A nondispersive infrared (NDIR) gas analyzer that utilizes a mid-infrared light emitting diode (LED) source was demonstrated for monitoring the metal alkylamide compound tetrakis(dimethylamido) titanium (TDMAT), Ti[N(CH3)2]4. This NDIR gas analyzer was based on direct absorption measurement of TDMAT vapor in the C-H stretching spectral region, a spectral region accessed using a LED with a nominal emission center wavelength of 3.65 μm. The sensitivity of this technique to TDMAT was determined by comparing the absorbance measured using this technique to the TDMAT density as determined using in situ Fourier transform IR (FT-IR) spectroscopy. Fourier transform IR spectroscopy was employed because this technique could be used to (1) quantify TDMAT density in the presence of a carrier gas (the presence of which precludes the use of a capacitance manometer to establish TDMAT density) and (2) distinguish between TDMAT and other gas-phase species containing IR-active C-H stretching modes (allowing separation of the signal from the LED-based optical system into fractions due to TDMAT and other species, when necessary). During TDMAT-only delivery, i.e., in the absence of co-reactants and deposition products, TDMAT minimum detectable molecular densities as low as ≈4 × 10(12) cm(-3) were demonstrated, with short measurement times and appropriate signal averaging. Reactions involving TDMAT often result in the evolution of the reaction product dimethylamine (DMA), both as a thermal decomposition product in a TDMAT ampoule and as a deposition reaction product in the deposition chamber. Hence, the presence of DMA represents a significant potential interference for this technique, and therefore, the sensitivity of this technique to DMA was also determined by measuring DMA absorbance as a function of pressure. The ratio of the TDMAT sensitivity to the DMA sensitivity was determined to be ≈6.0. To further examine the selectivity of this technique, measurements were also performed during atomic layer deposition (ALD) of titanium dioxide using TDMAT and water. During ALD, potential interferences were expected from the evolution of DMA due to deposition reactions and the deposition on the windows of species containing IR-active C-H stretching modes. It was found that the interfering effects of the evolution of DMA and deposition of species on the windows corresponded to a maximum of only ≈6% of the total observed TDMAT density. However, this level of interference likely is relatively low compared to a typical chemical vapor deposition process in which co-reactants are introduced into the chamber at the same time.

Download full-text PDF

Source
http://dx.doi.org/10.1366/14-07695DOI Listing

Publication Analysis

Top Keywords

tdmat density
16
tdmat
14
c-h stretching
12
deposition
9
metal alkylamide
8
atomic layer
8
layer deposition
8
diode led
8
led source
8
ndir gas
8

Similar Publications

A theoretical study on the surface reaction of tetrakis(dimethylamino)titanium on titanium oxide.

Phys Chem Chem Phys

August 2023

Metal-organic Compounds Materials Research Center, Sejong University, Seoul, 05006, Republic of Korea.

Tetrakis(dimethylamino)-titanium (TDMAT, Ti(NMe)) has been used for the low-temperature atomic layer deposition (ALD) process of titanium oxide (TiO) films. In this study, the chemisorption of TDMAT on a titanium oxide surface using a slab model was simulated by density functional theory (DFT) calculation. We calculated the activation energy for the chemisorption and predicted the final chemisorbed species.

View Article and Find Full Text PDF

Surface Defect Engineering of MoS for Atomic Layer Deposition of TiO Films.

ACS Appl Mater Interfaces

October 2020

Department of Physics, UMBC, Baltimore, Maryland 21250, United States.

In this manuscript, we combine experimental and computational approaches to study the atomic layer deposition (ALD) of dielectrics on MoS surfaces for a very common class of ALD precursors, the alkylamines. More specifically, we study the thermal ALD of TiO from TDMAT and HO. Depositions on as-produced chemical vapor deposition MoS flakes result in discontinuous films.

View Article and Find Full Text PDF

SiGe(110) surfaces were passivated and functionalized using atomic H, hydrogen peroxide (HO), and either tetrakis(dimethylamino)titanium (TDMAT) or titanium tetrachloride (TiCl) and studied in situ with multiple spectroscopic techniques. To passivate the dangling bonds, atomic H and HO(g) were utilized and scanning tunneling spectroscopy (STS) demonstrated unpinning of the surface Fermi level. The HO(g) could also be used to functionalize the surface for metal atomic layer deposition.

View Article and Find Full Text PDF

Molecular layer deposition (MLD) of hybrid organic-inorganic thin films called "titanicones" was achieved using tetrakisdimethylaminotitanium (TDMAT) and glycerol (GL) or ethylene glycol (EG) as precursors. For EG, in situ ellipsometry revealed that the film growth initiates, but terminates after only 5 to 10 cycles, probably because both hydroxyls react with the surface. GL has a third hydroxyl group, and in that case steady state growth could be achieved.

View Article and Find Full Text PDF

A nondispersive infrared (NDIR) gas analyzer that utilizes a mid-infrared light emitting diode (LED) source was demonstrated for monitoring the metal alkylamide compound tetrakis(dimethylamido) titanium (TDMAT), Ti[N(CH3)2]4. This NDIR gas analyzer was based on direct absorption measurement of TDMAT vapor in the C-H stretching spectral region, a spectral region accessed using a LED with a nominal emission center wavelength of 3.65 μm.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!