Effects of secondary phase and grain size on the corrosion of biodegradable Mg-Zn-Ca alloys.

Mater Sci Eng C Mater Biol Appl

School of Metallurgy and Materials, University of Birmingham, Edgbaston, Birmingham B15 2TT, United Kingdom.

Published: March 2015

The bio-corrosion behaviour of Mg-3Zn-0.3Ca (wt.%) alloy in simulated body fluid (SBF) at 37°C has been investigated using immersion testing and electrochemical measurements. Heat treatment has been used to alter the grain size and secondary phase volume fraction; the effects of these on the bio-corrosion behaviour of the alloy were then determined. The as-cast sample has the highest bio-corrosion rate due to micro-galvanic corrosion between the eutectic product (Mg+Ca2Mg6Zn3) and the surrounding magnesium matrix. The bio-corrosion resistance of the alloy can be improved by heat treatment. The volume fraction of secondary phases and grain size are both key factors controlling the bio-corrosion rate of the alloy. The bio-corrosion rate increases with volume fraction of secondary phase. When this is lower than 0.8%, the dependence of bio-corrosion rate becomes noticeable: large grains corrode more quickly.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.msec.2014.12.049DOI Listing

Publication Analysis

Top Keywords

bio-corrosion rate
16
secondary phase
12
grain size
12
volume fraction
12
bio-corrosion behaviour
8
heat treatment
8
fraction secondary
8
bio-corrosion
7
effects secondary
4
phase grain
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!