Graphene has been drawing worldwide attention since its discovery in 2004. In order to realize graphene-based devices, thin, uniform-coverage and pinhole-free dielectric films with high permittivity on top of graphene are required. Here we report the direct growth of Al2O3-doped HfO2 films onto graphene by H2O-based atom layer deposition (ALD). Al2O3-onto-HfO2 stacks benefited the doping of Al2O3 into HfO2 matrices more than HfO2-onto-Al2O3 stacks did due to the micro-molecular property of Al2O3 and the high chemical activity of trimethylaluminum (TMA). Al2O3 acted as a network modifier, maintained the amorphous structure of the film even to 800 °C, and made the film smooth with a root mean square (RMS) roughness of 0.8 nm, comparable to the surface of pristine graphene. The capacitance and the relative permittivity of Al2O3-onto-HfO2 stacks were up to 1.18 μF cm(-2) and 12, respectively, indicating the high quality of Al2O3-doped HfO2 films on graphene. Moreover, the growth process of Al2O3-doped HfO2 films introduced no detective defects into graphene confirmed by Raman measurements.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1039/c4cp04957h | DOI Listing |
Phys Chem Chem Phys
February 2015
State Key Laboratory of Functional Materials for Informatics, Institute of Microsystem and Information Technology, Chinese Academy of Sciences, Changning Road 865, Shanghai 200050, P. R. China.
Graphene has been drawing worldwide attention since its discovery in 2004. In order to realize graphene-based devices, thin, uniform-coverage and pinhole-free dielectric films with high permittivity on top of graphene are required. Here we report the direct growth of Al2O3-doped HfO2 films onto graphene by H2O-based atom layer deposition (ALD).
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!