The hierarchical architecture of protective biological materials such as mineralized fish scales, gastropod shells, ram's horn, antlers, and turtle shells provides unique design principles with potentials for guiding the design of protective materials and systems in the future. Understanding the structure-property relationships for these material systems at the microscale and nanoscale where failure initiates is essential. Currently, experimental techniques such as nanoindentation, X-ray CT, and SEM provide researchers with a way to correlate the mechanical behavior with hierarchical microstructures of these material systems1-6. However, a well-defined standard procedure for specimen preparation of mineralized biomaterials is not currently available. In this study, the methods for probing spatially correlated chemical, structural, and mechanical properties of the multilayered scale of A. spatula using nanoindentation, FTIR, SEM, with energy-dispersive X-ray (EDX) microanalysis, and X-ray CT are presented.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC4214185PMC
http://dx.doi.org/10.3791/51535DOI Listing

Publication Analysis

Top Keywords

fish scales
8
spatula nanoindentation
8
nanoindentation x-ray
8
ftir sem
8
characterization multi-layered
4
multi-layered fish
4
scales atractosteus
4
atractosteus spatula
4
x-ray
4
x-ray ftir
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!