In this study, a controllable photonic mirror was fabricated using the atomic layer deposition (ALD) coating technique on a polystyrene (PS) nanosphere template. PS nanospheres were self-assembled on an Al/glass substrate to form the bottom electrode. A 20 nm ALD Al2O3 film was then coated onto the surface of the reduced PS nanosphere structure. The PS nanospheres were removed in air at 350°C to form hollow Al2O3 nanospheres. Then a 30 nm indium tin oxide film was sputtered on the hollow nanosphere structure to form the top electrode. The results show that the incorporation of the photonic mirror could control the reflectance to a value of 0.3% per 0.1 V of bias voltage.

Download full-text PDF

Source
http://dx.doi.org/10.1364/AO.53.00A237DOI Listing

Publication Analysis

Top Keywords

photonic mirror
12
controllable photonic
8
mirror fabricated
8
fabricated atomic
8
atomic layer
8
layer deposition
8
nanosphere template
8
nanosphere structure
8
nanosphere
4
deposition nanosphere
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!