Three-unit CAD/CAM-generated lithium disilicate FDPs after a mean observation time of 46 months.

Clin Oral Investig

Department of Prosthodontics and Biomaterials, Centre of Implantology, Medical Faculty, RWTH Aachen University, Pauwelsstraße 30, 52074, Aachen, Germany,

Published: December 2014

Objectives: Lithium disilicate can easily be machined by CAM techniques in its metasilicate status. Due to slightly inferior material properties, the material is not yet recommended for three-unit fixed dental prosthesis (FDP) as it is the case for the press material up to the second bicuspid. Therefore, the aim of this clinical study was to evaluate the performance of CAD/CAM-fabricated lithium disilicate FDPs.

Materials And Methods: A total of 32 anterior and posterior FDPs were provided for 32 patients. Twelve FDPs were fabricated chair-side. The first recall took place 6 months after insertion and then annually. The FDPs were rated according to biological and technical complications. As failure, those events were defined, which led to the removal of a FDP. The failure-free (survival) rate and the complication-free rate were calculated according to Kaplan-Meier.

Results: After a mean observation time of 46 months (SD ± 8.4 months), three endodontic complications in two FDPs, two minor chippings, and one catastrophic fracture occurred. One FDP had to be removed due to persisting undefined complaints. Thus, the failure-free rate and the complication-free rate were revealed as 93 and 83 %, respectively.

Conclusions: Despite the limited observation period, the results are promising, especially due to the fact that the fractured FDP did not fulfill the recommended connector dimensions.

Clinical Relevance: Inserted as a full-contour three-unit FDP within its indications, the CAD/CAM lithium disilicate ceramic offers an appropriate alternative to layered restorations.

Download full-text PDF

Source
http://dx.doi.org/10.1007/s00784-014-1191-8DOI Listing

Publication Analysis

Top Keywords

lithium disilicate
16
observation time
8
time months
8
rate complication-free
8
complication-free rate
8
fdps
5
fdp
5
three-unit cad/cam-generated
4
lithium
4
cad/cam-generated lithium
4

Similar Publications

Objective: This study aimed to evaluate the chemical solubility (CS) and conduct a comprehensive physicochemical characterization of several experimental and commercial lithium silicate-based glass-ceramics towards an understanding of the chemical processes governing dissolution in these glass-ceramics.

Methodology: Glass-ceramic (GC) samples were categorized into two groups: experimental materials featuring lithium metasilicate crystals (GCE1 and GCE2); and five commercial brands relying mostly on lithium disilicate (Celtra®Duo, IPS e.max®CAD, Straumann®n!ce®, CEREC Tessera™, and VITA Suprinity®).

View Article and Find Full Text PDF

Effect of crystallization and finish line curvature on the marginal integrity of lithium disilicate crowns.

J Prosthodont

January 2025

Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University, Gangneung, South Korea.

Purpose: This study aimed to investigate the effect of crystallization and finish line curvature on the integrity of lithium disilicate crowns fabricated by using partially crystallized (P) and fully crystallized (F) blocks.

Materials And Methods: Forty-eight lithium disilicate crowns were fabricated based on the designated lithium disilicate blocks and finish line curvatures. The specimens were divided into four groups (n = 12 each): P block with a curved finish line (PC), P block with a straight finish line (PS), F block with a curved finish line (FC), and F block with a straight finish line (FS).

View Article and Find Full Text PDF

Objective: The objective of this study was to evaluate and compare the fracture resistance of MOD inlay preparations restored with two different lithium disilicate glass ceramics.

Materials And Methods: Standardized MOD inlay cavities were prepared on 64 human permanent premolar teeth and divided into two groups to be restored with lithium disilicate glass-ceramic materials, i.e.

View Article and Find Full Text PDF

Objective: To conduct a systematic review on the masking ability of subtractively and additively manufactured dental ceramics.

Materials And Methods: The study followed the Preferred Reporting Items for Systematic Reviews and Meta-Analyses (PRISMA) statement. The electronic search was carried out through MEDLINE, Scopus, and Website of Science databases with a date restriction being from 2001 onwards.

View Article and Find Full Text PDF

This study evaluated the survival probabilities of two lithia-based glass-ceramics after final crystallization in a microwave furnace using conventional crystallization as a reference. Disc-shaped samples of a lithium silicate (LS, Celtra Duo) and a lithium disilicate (LD, e.max CAD) were prepared and divided into two groups according to the crystallization method (n = 30): microwave (M) or conventional furnaces (C).

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!