Aim: The aim of the study is to investigate the galvanic corrosion potential of metal injection molding (MIM) brackets to that of conventional brackets under similar in vitro conditions with nickel-titanium and copper nickel-titanium archwires.
Materials And Methods: Twenty-five maxillary premolar MIM stainless steel brackets and 25 conventional stainless steel brackets and archwires, 0.16 inch, each 10 mm length, 25 nickeltitanium wires, 25 copper nickel-titanium wires were used. They were divided into four groups which had five samples each. Combination of MIM bracket with copper nickel-titanium wire, MIM bracket with nickel-titanium wire and conventional stainless steel brackets with copper nickel-titanium wire and conventional stainless steel brackets with nickel-titanium wires which later were suspended in 350 ml of 1 M lactic acid solution media. Galvanic corrosion potential of four groups were analyzed under similar in vitro conditions. Precorrosion and postcorrosion elemental composition of MIM and conventional stainless steel bracket by scanning electron microscope (SEM) with energy dispersive spectroscope (EDS) was done.
Results: MIM bracket showed decreased corrosion susceptibility than conventional bracket with copper nickeltitanium wire. Both MIM and conventional bracket showed similar corrosion resistance potential in association with nickel-titanium archwires. It seems that both brackets are more compatible with copper nickel-titanium archwires regarding the decrease in the consequences of galvanic reaction. The EDS analysis showed that the MIM brackets with copper nickel-titanium wires released less metal ions than conventional bracket with copper nickeltitanium wires.
Conclusion: MIM brackets showed decreased corrosion susceptibility, copper nickel-titanium archwires are compatible with both the brackets than nickel-titanium archwires.
Clinical Significance: Clinically MIM and conventional brackets behaved more or less similarly in terms of corrosion resistance. In order to decrease the corrosion potential of MIM brackets, more precise manufacturing technique should be improved to get a more smoother surface finish.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.5005/jp-journals-10024-1350 | DOI Listing |
Biofabrication
January 2025
Mechanical Engineering, National Institute of Technology Meghalaya, Shillong, Shillong, Meghalaya, 793003, INDIA.
The process of micromachining has garnered attention for its ability to create three-dimensional tiny features, particularly in ultra-hard and exotic materials. The present work investigates the effect of different parameters of the µ-ED milling, such as pulse on time (Ton), pulse off time (Toff), voltage (V), and tool rotation (TR) on the dimensional deviation (DD), material removal rate (MRR), surface roughness (Ra), and machined surface characteristics (analysed by EDS and FESEM). The sesame oil as dielectric and tungsten-copper as tool electrodes were used to maintain the accuracy and improve the machinability of bio-grade Nitinol SMA.
View Article and Find Full Text PDFJ Orthod Sci
November 2024
Department of Orthodontics, Indira Gandhi Institute of Dental Sciences, Pondicherry, India.
Background/objective: Resolution of crowding remains a chief concern for patients seeking orthodontic treatment. The choice of the initial aligning archwire is crucial for achieving treatment success. Nickel-titanium (NiTi) archwires have been the first choice since their introduction.
View Article and Find Full Text PDFCardiovasc Pathol
December 2024
University Hospital Muenster, Department of Cardiothoracic Surgery, Muenster, Germany.
Objectives: Re-operations due to material degeneration carry a burden for patients with congenital heart disease (CHD). The study aim was to compare rapid vs. slow degeneration of biomaterials in CHD patients.
View Article and Find Full Text PDFContraception
November 2024
Department of Obstetrics and Gynecology, University of Utah School of Medicine, Salt Lake City, UT, USA. Electronic address:
Objectives: This study aimed to assess 3-year efficacy, safety, and tolerability of the Cu 175 mm intrauterine device (IUD).
Study Design: This single-arm trial recruited participants at risk of pregnancy aged 17 to 45 years at 42 U.S.
Orthod Fr
November 2024
Département d’Orthodontie, Faculté de Médecine dentaire, Université Saint-Joseph, 650 rue de Damas, B.P. 11-5076 Riad El Solh, Beyrouth, Liban
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!