The strength retention characteristics of oriented semicrystalline polylactides were monitored during hydrolytic degradation in vitro. The effects of the polymer type, the material's initial inherent viscosity (iv), the sample diameter and the residual monomer content on strength retention were analyzed. The analyzed polylactides had similar, but not identical, strength retention characteristics. It was concluded that a higher degree of initial crystallinity was a major variable determining the earlier and more profound strength loss of PLLA than 96L/4D PLA and 80L/20 D,L PLA. Samples with a higher initial iv were found to have a longer strength retention time than lower iv samples. Size-dependency was observed, as the strength retention time was shorter for the smaller diameter samples. This size-dependency was caused by faster iv decay. The amount of residual monomer content had a remarkable impact on strength retention. Neither the sample diameter, initial iv or residual monomer content were found to have an effect on the iv range in which there was a rapid decline in strength properties. Therefore, it was concluded that the inherent viscosity and/or molecular weight of oriented PLLA, 96L/4D PLA and 80L/20 D,L PLA is a major variable determining the strength retention of these materials.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC3825234PMC
http://dx.doi.org/10.4161/biom.26395DOI Listing

Publication Analysis

Top Keywords

strength retention
32
plla 96l/4d
12
96l/4d pla
12
residual monomer
12
monomer content
12
strength
10
oriented plla
8
retention characteristics
8
inherent viscosity
8
sample diameter
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!