The purpose of this study was to evaluate the effect of air-blowing duration on the bonding performance of all-in-one systems using the same pressure (0.25 MPa). Three all-in-one systems were: EB (Easy Bond, 3M ESPE, USA), BB (BeautiBond, Shofu Inc., Japan) and GBp (G-Bond plus, GC Corporation, Japan). After adhesive application, the 3 systems were air-blown thereafter using 7 different durations (5 s, 10 s, 15 s, 20 s, 25 s, 30 s and 35 s). Bond strengths to dentin were determined using µTBS test after 24 h water storage. In addition, evaluation of both the resin-dentin interface and the fractured surface on the dentin side were performed by SEM. The maximum µTBS for each system, BB (40.4±14.8 MPa), EB (79.8±16.5 MPa), and GBp (47.3±17.6 MPa), were recorded with 15 s, 15 s and 25 s air-blowing duration respectively. Under the same air-pressure, the air-blowing duration could affect evaporation and the thickness of the adhesive layer, which contributed to the different bond strengths.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.4012/dmj.2012-205 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!