Objective: To study the corrosion resistance of casted titanium by plasma nitriding and TiN-coated compound treatments in the artificial saliva with different fluoride concentrations and to investigate whether compound treatments can increase the corrosion resistance of casted titanium.

Methods: Potentiodynamic polarization technique was used to depict polarization curve and to measured the current density of corrosion (Icorr) and the electric potential of corrosion (Ecorr) of casted titanium (Group A) and casted titanium by compound treatments (Group B) in the artificial saliva with different fluoride concentrations. After electrochemical experiment, the microstructure was observed by scanning electron microscope (SEM).

Results: The Icorrs of Group A and B in the artificial saliva of different fluoride concentrations were (1530.23 ± 340.12), (2290.36 ± 320.10), (4130.52 ± 230.17) nA and (2.62 ± 0.64), (7.37 ± 3.59), (10.76 ± 6.05) nA, respectively. The Ecorrs were (-0.93 ± 0.10), (-0.89 ± 0.21), (-0.57 ± 0.09) V and (-0.21 ± 0.04), (-0.17 ± 0.03), (-0.22 ± 0.03) V, respectively.The Icorrs of Group B were significantly lower (P < 0.01)than that of Group A. The Icorrs increased significantly with the increasing of fluoride concentrations (P < 0.01). The Ecorrs of Group B were significantly higher than that of Group A (P < 0.01). The SEM confirmed the microstructure in the casted titanium was much severely than that in Group B, the microstructure in Group A and B corroded more and more heavily with increasing of fluoride concentrations.

Conclusions: The increase of fluoride concentrations influence the corrosion resistance of both treated and untreated casted titanium negatively, but plasma nitriding and TiN-coated compound treatments can significantly increase the corrosion resistance of casted titanium.

Download full-text PDF

Source
http://dx.doi.org/10.3760/cma.j.issn.1002-0098.2012.09.012DOI Listing

Publication Analysis

Top Keywords

casted titanium
28
compound treatments
20
fluoride concentrations
20
resistance casted
16
artificial saliva
16
saliva fluoride
16
corrosion resistance
16
group
9
casted
8
titanium compound
8

Similar Publications

In-vitro investigation of chitosan/polyvinyl alcohol/TiO composite membranes for wound regeneration.

Biochem Biophys Res Commun

January 2025

Department of Physics, School of Advanced Sciences, Vellore Institute of Technology, Vellore, 632014, India. Electronic address:

Bacterial infections significantly delay the physiological wound healing process and can cause further damage to the wound region. In the current work, we aim to design titanium dioxide nanoparticles (TiO NPs) incorporated with chitosan (Chi) and poly (vinyl alcohol) (PVA) film using the casting method and to study their potential for faster wound healing. The prepared TiO NPs were analyzed for physicochemical properties, and TEM results showed an average particle size of 39.

View Article and Find Full Text PDF

Antimicrobial effects of pulsed light activated TiO-Polylactic acid film.

Heliyon

October 2024

Eastern Regional Research Center, Agricultural Research Service, U.S. Department of Agriculture, 600 East Mermaid Lane, Wyndmoor, PA, 19038, USA.

Article Synopsis
  • A study evaluated the antimicrobial properties of TiO incorporated polylactic acid (PLA) films activated by pulsed light (PL), using different ratios of TiO/PLA.
  • The films were tested for their effectiveness against bacteria after various PL treatments, revealing significant reductions in bacterial populations, especially with a 5-second PL treatment.
  • Results showed that the TiO-PLA films maintained their antibacterial activity for 2 hours post-treatment, indicating their potential use in food packaging applications sensitive to UV light.
View Article and Find Full Text PDF

Background: The accuracy of digital implant transfer is currently under investigation in relation to the effect of saliva, scan body material, and exposed length.

Methods: Six completely edentulous casts with four implant fixtures were fabricated. The four implant fixtures in each cast were placed below the crest of the ridge of the casts by 1.

View Article and Find Full Text PDF

Cranial reconstruction utilizing polymeric implants in two different designs: finite element investigation.

BMC Musculoskelet Disord

November 2024

Biomedical Engineering Department, Faculty of Engineering, Helwan University, Cairo, Egypt.

Introduction: Impact loads applied to the human head can result in skull fractures or other injuries that require a craniectomy. The removed portion is replaced with biological or synthetic materials using cranioplasty surgery. Titanium has been the material of choice for cranial implants due to its superior properties and biocompatibility; however, its issues have prompted the search for substitute materials (e.

View Article and Find Full Text PDF

Direct detection of melamine in milk via surface-enhanced Raman scattering using gold-silver anisotropic nanostructures.

Spectrochim Acta A Mol Biomol Spectrosc

February 2025

Center for Advanced Materials Research, Research Institute of Sciences and Engineering, University of Sharjah, PO Box 27272, Sharjah, United Arab Emirates; Department of Applied Physics and Astronomy, University of Sharjah, PO Box 27272, Sharjah, United Arab Emirates.

Article Synopsis
  • The study focuses on creating anisotropic gold-silver nanoparticles (a-AuAg) coated on titanium sheets to improve Surface-enhanced Raman Spectroscopy (SERS) for detecting harmful milk adulterants like melamine.
  • These a-AuAg nanoparticles exhibit unique shapes (triangular, hexagonal, pentagonal) that significantly enhance SERS performance, showing a 1.7 x 10 improvement in sensitivity compared to regular spherical nanoparticles.
  • The detection limits for melamine were found to be very low in spiked samples, with a higher sensitivity compared to traditional methods, although tested commercial milk products did not show detectable melamine.
View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!