A description is given of the design and performance of a diagnostic-accessible, perpendicular-flow, single-wafer deposition reactor for use with 50 mm wafers. The reactor chamber design is based on a simple flow tube, with diagnostic access achieved by replacing sections of the reactor chamber wall with recessed diagnostic ports. Reactor chamber performance is evaluated for the purpose of performing optical measurements during atomic layer deposition (ALD). Computational fluid dynamics simulations predict that the when used with windows the diagnostic port design produces minimal perturbations to the gas flow under typical deposition conditions, as compared to a design without diagnostic ports. Temperature measurements of the inside surface of a window installed in a diagnostic port suggest that for reactor chamber operation at 110 °C, under typical deposition conditions, the inside surface window temperature is approximately equal to or greater than the surrounding reactor chamber temperature, thereby minimizing possible species condensation on the window surface. As a consequence of using recessed diagnostic ports, an increase in the amplitude of optical intensity fluctuations was generally observed when performing measurements at elevated chamber temperatures. These intensity fluctuations could be readily reduced by enclosing the optical path to the exterior side of the windows. The performance of two straight-forward methods to reduce these intensity fluctuations is presented. The results outlined above demonstrate that this reactor design can be operated with short gas residence times and with all reactor surfaces at elevated temperatures, making it useful for simulating a wide range of gas flow conditions with relevance to microelectronics-related ALD processes.

Download full-text PDF

Source
http://dx.doi.org/10.1063/1.4742991DOI Listing

Publication Analysis

Top Keywords

reactor chamber
24
diagnostic ports
12
intensity fluctuations
12
reactor
9
perpendicular-flow single-wafer
8
atomic layer
8
layer deposition
8
deposition reactor
8
chamber design
8
recessed diagnostic
8

Similar Publications

CFD modelling and simulations of atomization-based processes for production of drug particles: A review.

Int J Pharm

January 2025

SSPC Research Centre, Department of Chemical Sciences & Chemical Engineering, Bernal Institute, University of Limerick, Limerick V94 T9PX Ireland. Electronic address:

Atomization-based techniques are widely used in pharmaceutical industry for production of fine drug particles due to their versatility and adaptability. Key performance measure of such techniques is their ability to provide control over critical quality attributes (CQAs) of produced drug particles. CQAs of drug particles produced via atomization critically depend on fluid dynamics of sprays; resulting mixing, heat and mass transfer; distribution of supersaturation and subsequent nucleation and growth of particles.

View Article and Find Full Text PDF

Evaluation of the Wear of Ni 200 Alloy After Long-Term Carbon Capture in Molten Salts Process.

Materials (Basel)

December 2024

Department of Geomechanics, Civil Engineering and Geotechnics, Faculty of Civil Engineering and Resource Management, AGH University of Krakow, al. Adama Mickiewicza 30, 30-059 Cracow, Poland.

Reducing CO emissions is one of the major challenges facing the modern world. The overall goal is to limit global warming and prevent catastrophic climate change. One of the many methods for reducing carbon dioxide emissions involves capturing, utilizing, and storing it at the source.

View Article and Find Full Text PDF

Evaluating the Appropriateness of Selected Foundry Sands for the Casting of Reactor Housings: A Study Based on Physicochemical Characterization Outcomes.

Materials (Basel)

December 2024

Faculty of Geology, Geophysics and Environmental Protection, AGH University of Krakow, al. A. Mickiewicza 30, 30-059 Krakow, Poland.

In the case of desulfurization and spheroization of cast iron using the in-mold method, in which the treated cast iron is poured into the reaction chamber and placed in the casting mold, the mineral raw material of the mold should support these processes. Therefore, it is important to know the physicochemical properties of the materials selected for the production of casting molds and to learn about the phenomena occurring during their pouring. The research presented in this paper was carried out on quartz, magnesite, chromite, and olivine sands.

View Article and Find Full Text PDF

Assessment of air pollutant O pulmonary exposure using a bronchus-on-chip model coupling with atmospheric simulation chamber.

J Hazard Mater

January 2025

Laboratory of Atmospheric Environment and Pollution Control (LAEPC), Research Center for Eco-Environmental Sciences, Chinese Academy of Sciences, Beijing 100085, China; College of Resources and Environment, University of Chinese Academy of Sciences, Beijing 100049, China. Electronic address:

Heavy air pollution is now a serious public health issue. Many studies have shown strong connections between ozone (O) with the occurrence and development of various respiratory diseases. However, the exact mechanism is still a matter of debate.

View Article and Find Full Text PDF

In soil polluted with benzene, toluene, ethylbenzene, and xylenes (BTEX), oxygen is rapidly depleted by aerobic respiration, creating a redox gradient across the plume. Under anaerobic conditions, BTEX biodegradation is then coupled with fermentation and methanogenesis. This study aimed to characterize this multi-step process, focusing on the interactions and functional roles of key microbial groups involved.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!