Sulfate-reducing bacteria lower sulfur-mediated pitting corrosion under conditions of oxygen ingress.

Environ Sci Technol

Petroleum Microbiology Research Group, Department of Biological Sciences, University of Calgary, 2500 University Drive NW, Calgary, Alberta T2N 1N4, Canada.

Published: August 2012

The effect of oxygen ingress into sour water containing dissolved sulfide on the production of sulfur and polysulfide (S-PS) and associated iron corrosion was investigated. Biotic (active SRB present), abiotic (autoclaved SRB present), and chemical (no bacteria present) conditions were compared. Under biotic conditions formation of S-PS was only seen at a high ratio of oxygen to sulfide (R(OS)) of 1 to 2.4. General corrosion rates increased 10-fold to 0.10 mm/yr under these conditions. Under abiotic and chemical conditions S-PS formation increased over the entire range of R(OS) with general corrosion rates reaching 0.06 mm/yr. Although general corrosion rates were thus highest under biotic conditions, biotically corroded coupons showed much less pitting corrosion. Maximum pit depth increased to 40-80 μm with increasing R(OS) for coupons incubated for 1 month under abiotic or chemical conditions but not for biotically incubated coupons (10 μm). This appeared to be related to the properties and size of the sulfur formed, which was hydrophobic and in excess of 10 μm under chemical or abiotic conditions and hydrophilic and 0.5 to 1 μm under biotic conditions. Hence, perhaps contrary to expectation, SRB lowered pitting corrosion rates under conditions of oxygen ingress due to their ability to respire oxygen and produce a less aggressive form of sulfur. Microbial control, which is usually required in sour systems, may be counterproductive under these conditions.

Download full-text PDF

Source
http://dx.doi.org/10.1021/es3019594DOI Listing

Publication Analysis

Top Keywords

corrosion rates
16
pitting corrosion
12
oxygen ingress
12
biotic conditions
12
general corrosion
12
conditions
11
conditions oxygen
8
ros general
8
abiotic chemical
8
chemical conditions
8

Similar Publications

Agricultural waste or agro-waste, including natural fibers and particles from various crop parts, is increasingly recognized as a significant contributor to environmental issues. However, from a circular economy perspective, these materials present an opportunity to be repurposed into new, eco-friendly products. The present study, specifically focuses on understanding the effect of different factors, such as the particulate loading and the size (coir and hBN - 1 to 5 wt%; Coir Powder size (100-200 μm) of the particles on composite's corrosion rates and water absorption properties.

View Article and Find Full Text PDF

The objective of the study was to synthesize tetrazole molecules featuring nitro groups positioned at the para and meta locations. We aimed to assess their effectiveness in inhibiting corrosion of mild steel in a 1 M HCl solution at 298 K. Tetrazoles with 2,5-disubstitution were created using [3 + 2] cycloaddition and N-alkylation techniques, with a particular emphasis on synthesizing molecules that contain nitro groups.

View Article and Find Full Text PDF

High-voltage transmission lines face significant challenges due to environmental exposure, including corona discharge, ice accretion, and corrosion, which impact their durability and operational efficiency. This study investigates the performance of hydrophilic and superhydrophilic organosilane coatings applied to high-voltage wires to address these issues. Using a combination of experimental setups simulating real-world conditions, we evaluated corona discharge losses, ice adhesion, and corrosion resistance on coated and uncoated wires.

View Article and Find Full Text PDF

Perfluorononanoic acid (PFNA), widely employed in surfactants, coatings, plastics, corrosion inhibitors, and fire-extinguishing agents, is less regulated than PFOS or PFOA but displays higher bioaccumulation and potential toxicity. Most toxicity assessments have focused on mammals, fish, and algae, with limited research on ground-dwelling arthropods, especially ants. Here, we examined PFNA's toxic effects on red imported fire ants (RIFAs), a prevalent ground-dwelling species in South China.

View Article and Find Full Text PDF

Human papillomavirus (HPV) infections rank as the most prevalent sexually transmitted infections globally. The Brazilian Ministry of Health recommends the topical use of 70%-90% trichloroacetic acid (TAA) for treating condyloma acuminata, yet this method suffers from a high recurrence rate of 36% and requires roughly six applications. Topical photodynamic therapy (PDT) has shown effectiveness in targeting subclinical lesions, but it also necessitates multiple sessions for complete lesion clearance.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!