Purpose: The purpose of this systematic review was to compare the survival and complication rates of ceramic veneers produced with different techniques and materials after a minimum follow-up time of 5 years.

Materials And Methods: A literature search was conducted, using electronic databases, relevant references, citations and journal researching, for clinical studies reporting on the survival of ceramic veneers fabricated with different techniques and materials with a mean followup time of at least 5 years. The search period spanned from January 1980 up to October 2010. Event rates were calculated for the following complications associated with ceramic veneers: fracture, debonding, marginal discoloration, marginal integrity, and caries. Summary estimates, and 5-year event rates were reported. Comparison between subgroups of different materials, as well as statistical significance, was calculated using a mixed effects model.

Results: Nine studies were selected for final analysis over an initial yield of 409 titles. No study directly compared the incidence of complications between ceramic veneers fabricated from different materials. Four of the included studies reported on the survival of ceramic veneers made out of feldspathic ceramics; four studies were on glass-ceramic veneers and one study included veneers fabricated from both materials. The mean observation time ranged between 5 and 10 years. Overall, the 5-year complication rates were low, with the exception of studies reporting on extended ceramic veneers. The most frequent complication reported was marginal discoloration (9% at 5 years), followed by marginal integrity (3.9-7.7% at 5 years). There was no statistically significant difference in the event rates between the subgroups of different materials (feldspathic vs. glass-ceramic).

Conclusion: The results of this systematic review showed that ceramic veneers fabricated from feldspathic or glass-ceramics have an adequate clinical survival for at least 5 years of clinical service, with very low complication rates.

Download full-text PDF

Source

Publication Analysis

Top Keywords

ceramic veneers
32
veneers fabricated
16
survival ceramic
12
systematic review
12
complication rates
12
event rates
12
veneers
10
materials minimum
8
minimum follow-up
8
techniques materials
8

Similar Publications

Objective: This case report presents the interdisciplinary retreatment of a patient with a worn full-mouth rehabilitation using defect-oriented restorations, horizontal preparations, and vertical dimension of occlusion (VDO) increase.

Clinical Considerations: A 58-year-old woman with a previous full-mouth rehabilitation presented with worn dentition, loss of VDO, and reduced posterior support. Examination revealed signs of parafunctional habits, tetracycline-stained teeth, and compromised aesthetics with exposed discolored teeth and open embrasure spaces.

View Article and Find Full Text PDF

Purpose: To evaluate the shear bond strength (SBS) of stereolithography (SLA), digital light processing (DLP) manufactured, and computer numerical control (CNC) milled zirconia to veneering ceramic.

Materials And Methods: Rectangular shaped zirconia substrates (10 × 5 × 5 mm) were manufactured through SLA, DLP, and CNC technology separately. Their surface roughness was measured and the surface topography was analyzed by atomic force microscope (AFM).

View Article and Find Full Text PDF

Background: The growing demand for esthetic restorative materials highlights the need to evaluate their marginal accuracy and fracture resistance to ensure optimal clinical outcomes for primary molars.

Aim: The aim was to assess the vertical marginal gap distance and fracture resistance of esthetic restorative materials after cyclic loading.

Design: Forty extracted primary molars were randomly divided into four groups: Group I, stainless steel veneered crowns with tooth-colored material; Group II, prefabricated monolithic zirconia crowns; Group III, yttria-partially stabilized zirconia computer-aided design/computer-aided manufacturing (CAD/CAM) crowns; and Group IV, hybrid ceramic CAD/CAM crowns.

View Article and Find Full Text PDF

Wear Resistance of Light-Cure Resin Luting Cements for Ceramic Veneers.

J Funct Biomater

December 2024

Department of Operative Dentistry, School of Dentistry, Aichi Gakuin University, Nagoya 464-8651, Japan.

The purpose of this study was to compare the wear resistance of light-cure resin luting cements for veneers with that of other luting materials investigated in earlier studies. An Alabama wear-testing machine was used to measure the wear resistance of four recent light-cure resin luting cements for veneers (G-Cem Veneer; Panavia V5 LC; RelyX Veneer Cement; and Vario-link Esthetic LC). The volume loss ranged from 0.

View Article and Find Full Text PDF

The injection moulding technique (IMT) is a minimally invasive restorative treatment. This technique enables the application of thin, flowable composite layers into a stable, transparent silicone index that serves as a mould. Due to the fluid properties of the composite, it efficiently fills the silicone tray and seamlessly integrates with the tooth structure, often obviating tooth preparation and preserving overall tooth integrity.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!