Effects of design and materials on the dielectrophoretic self-assembly of individual gallium nitride nanowires (GaN NWs) onto microfabricated electrodes have been experimentally investigated. The use of TiO(2) surface coating generated by atomic layer deposition (ALD) improves dielectrophoretic assembly yield of individual GaN nanowires on microfabricated structures by as much as 67%. With a titanium dioxide coating, individual nanowires were placed across suspended electrode pairs in 46% of tests (147 out of 320 total), versus 28% of tests (88 out of 320 total tests) that used uncoated GaN NWs. An additional result from these tests was that suspending the electrodes 2.75 μm above the substrate corresponded with up to 15.8% improvement in overall assembly yield over that of electrodes fabricated directly on the substrate.

Download full-text PDF

Source
http://dx.doi.org/10.1088/0957-4484/23/24/245301DOI Listing

Publication Analysis

Top Keywords

atomic layer
8
layer deposition
8
microfabricated electrodes
8
gan nws
8
assembly yield
8
320 total
8
controlled dielectrophoretic
4
dielectrophoretic nanowire
4
nanowire self-assembly
4
self-assembly atomic
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!