The purpose of this study was to analyze the effect of strontium-substituted hydroxyapatite (Sr-HA) on bone osseointegration of the implants using fluorescence microscopy. We allocated 20 implants to two groups: Sr-HA group and HA group. Electrochemically deposited HA and Sr-HA coatings were applied onto the implants separately. All the implants were inserted into femur bone of rabbits. Oxytetracycline hydrochloride, alizarin-complexon, and calcein green were respectively administered 7, 28, and 46 d after the implantation. After eight weeks, femurs were retrieved and prepared for the fluorescence microscopy observation. We analyzed the bone mineral apposition rates (MARs), bone area ratios (BARs), and bone to implant contact (BIC) of the two groups. Fluorescence microscopic observation showed that all groups exhibited extensive early peri-implant bone formation. The MAR of the Sr-HA group was greater than that for pure HA from 7 to 28 d after implantation, but no significant difference was found at later stage. And the BIC showed difference at 7 and 28 d compared with pure HA. We concluded that Sr-HA coating can improve the bone osseointegration of the implant in the early stage compared with the HA coating.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC3348227 | PMC |
http://dx.doi.org/10.1631/jzus.B1100381 | DOI Listing |
J Dent Res
January 2025
Center for MicroElectroMechanical Systems, Universidade do Minho, Guimarães, Portugal.
In the present in vitro study, we evaluated the adhesion of an injectable platelet-rich fibrin (i-PRF) to laser-textured zirconia surfaces and their resultant friction behavior against bone tissue. Three types of zirconia surfaces were compared regarding the i-PRF coating effects: 1) grit blasted with 250-μm spherical alumina particles and acid etched with 20% hydrofluoric acid (ZLA), 2) laser textured with a random (RD) surface pattern, or 3) laser textured with a designed pattern based on 16 lines and 8 passages (L16N8). The coefficient of friction (COF) of the specimens was assessed on a reciprocating sliding pin-on-plate tribometer at 1-N normal load, 1 Hz, and a 2-mm stroke length.
View Article and Find Full Text PDFJ Prosthodont
January 2025
Department of Clinical and Biological Sciences, University of Turin, Turin, Italy.
Purpose: Few studies have explored the bone response in dental implant sites prepared using a piezoelectric device, indicating moderate effectiveness in enhancing secondary stability and osteogenesis. This study seeks to expand our understanding of the changes in biological, clinical, and radiographic parameters, during the initial phases of osseointegration in sites prepared with piezoelectric surgery.
Materials And Methods: Two implant sites were prepared in the tibia of four minipigs.
J Dent Sci
January 2025
School of Dental Technology, College of Oral Medicine, Taipei Medical University, Taipei, Taiwan.
Background/purpose: Early osseointegration of titanium (Ti) dental implants relies on the surface topography. Surface modification of Ti seeks to enhance bone regeneration around implants. Acid etching is the simple, less technique sensitive and cost-effective technique for surface treatment.
View Article and Find Full Text PDFJ Dent Sci
January 2025
Weintraub Center for Reconstructive Biotechnology, UCLA School of Dentistry, Los Angeles, CA, USA.
Background/purpose: studies are essential for understanding cellular responses, but traditional culture systems often neglect the three-dimensional (3D) structure of real implants, leading to limitations in cellular recruitment and behavior largely governed by gravity. The objective of this study was to pioneer a novel 3D dynamic osteoblastic culture system for assessing the biological capabilities of dental implants in a more clinically and physiologically relevant manner.
Materials And Methods: Rat bone marrow-derived osteoblasts were cultured in a 24-well dish with a vertically positioned dental implant.
J Dent Sci
January 2025
School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei, Taiwan.
Background/purpose: Osseointegration potential is greatly depended on the interaction between bone cells and dental implant surface. Since zirconia ceramic has a bioinert surface, functionalization of the surface with an organic compound allylamine was conducted to overcome its drawback of minimal interaction with the surrounding bone.
Materials And Methods: The zirconia surface was initially treated with argon glow discharge plasma (GDP), then combined with amine plasma at three different conditions of 50-W, 75-W and 85-W, to prepare the final samples.