Release of monomers from four different composite materials after halogen and LED curing.

Am J Dent

Department of Operative Dentistry and Periodontology, University Medical Center Freiburg, Dental School and Hospital, Hugstetter Strasse 55, 79106 Freiburg, Germany.

Published: October 2011

Purpose: To evaluate the release of monomers from four different composite materials (Ceram X, Filtek Supreme XT, Tetric Flow, Tetric EvoCeram), polymerized using either halogen or LED unit.

Methods: Ten specimens were made for each material/unit combination. Each specimen was stored in 1 ml 75% ethanol. The storage medium was renewed after 1, 7 and 28 days. Aliquots of this medium were analyzed by LC-MS/MS.

Results: The effect of the curing unit on monomers' release differed significantly among the materials (P < 0.0001). The amount of BisGMA and TEGDMA released from Ceram X was not influenced by the unit used (P > 0.05). Curing with LED reduced the amount of Bisphenol A released from Ceram X compared to halogen. For Filtek Supreme XT, the type of unit exerted a significant effect on the elution of BisGMA (P < or = 0.05). LED curing resulted in a higher release of TEGDMA and UDMA compared to halogen (P < or = 0.05). For Tetric Flow, LED curing resulted in lower monomer release (P < 0.0001). For Tetric EvoCeram, the amounts of BisGMA, UDMA and Bisphenol A were higher when polymerizing with LED compared to halogen. The release of substances was more material dependent and less influenced by the curing unit used.

Download full-text PDF

Source

Publication Analysis

Top Keywords

led curing
12
compared halogen
12
release monomers
8
monomers composite
8
composite materials
8
halogen led
8
filtek supreme
8
tetric flow
8
tetric evoceram
8
curing unit
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!