Zinc oxide (ZnO) nanoparticles were synthesized by a reaction between an aqueous-alcoholic solution of zinc nitrate and sodium hydroxide under ultrasonic irradiation at room temperature. The morphology, optical properties of the ZnO nanoparticles were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and UV-vis spectroscopy. The [60]fullerene and zinc oxide nanocomposite were synthesized in an electric furnace at 700 degrees C for two hours. The [60]fullerene-ZnO nanocomposite was characterized by XRD, SEM and TEM. In addition, the [60]fullerene-ZnO nanocomposite was investigated as a catalyst in the photocatalytic degradation of organic dyes using UV-vis spectroscopy. The photocatalytic activity of the [60]fullerene-ZnO nanocomposite was compared with that of ZnO nanoparticles, heated ZnO nanoparticles after synthesis, pure [60]fullerene, and heated pure [60]fullerene in organic dyes such as methylene blue (MB), methyl orange (MO), and rhodamine B (RhB) under ultraviolet light at 254 nm.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1166/jnn.2011.4374 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!