In vivo oxide-induced stress corrosion cracking of Ti-6Al-4V in a neck-stem modular taper: Emergent behavior in a new mechanism of in vivo corrosion.

J Biomed Mater Res B Appl Biomater

Syracuse Biomaterials Institute and Department of Biomedical and Chemical Engineering, Syracuse University, Syracuse, New York.

Published: February 2012

In vivo modular taper corrosion in orthopedic total joint replacements has been documented to occur for head-neck tapers, modular-body tapers, and neck-stem tapers. While the fretting corrosion mechanism by which this corrosion occurs has been described in the literature, this report shows new and as yet unreported mechanisms at play. A retrieved Ti-6Al-4V/Ti-6Al-4V neck-stem taper interface, implanted for 6 years is subjected to failure analysis to document taper corrosion processes that lead to oxide driven crack formation on the medial side of the taper. Metallurgical sectioning techniques and scanning electron microscopy analysis are used to document the taper corrosion processes. The results show large penetrating pitting attack of both sides of the taper interface where corrosion selectively attacks the beta phase of the microstructure and eventually consumes the alpha phase. The pitting attack evolves into plunging pits that ultimately develop into cracks where the crack propagation process is one of corrosion resulting in oxide formation and subsequent reorganization. This process drives open the crack and advances the front by a combination of oxide-driven crack opening stresses and corrosion attack at the tip. The oxide that forms has a complex evolving structure including a network of transport channels that provide access of fluid to the crack tip. This emergent behavior does not appear to require continued fretting corrosion to propagate the pitting and cracking. This new mechanism is similar to stress corrosion cracking where the crack tip stresses arise from the oxide formation in the crack and not externally applied tensile stresses.

Download full-text PDF

Source
http://dx.doi.org/10.1002/jbm.b.31943DOI Listing

Publication Analysis

Top Keywords

corrosion
12
taper corrosion
12
stress corrosion
8
corrosion cracking
8
modular taper
8
emergent behavior
8
fretting corrosion
8
taper interface
8
analysis document
8
document taper
8

Similar Publications

Chloride-induced corrosion of steel rebars embedded in mortar was effectively controlled by blending of gallic acid in wet mixture. Mixing of optimized concentration of gallic acid (GA) inhibitor (0.125%) in mortars considerably increased the charge transfer resistance of embedded rebars (80.

View Article and Find Full Text PDF

Safe and Sustainable by Design (SSbD) is a new regulatory concept guiding chemical and material innovation. The European Commission has recommended a two-stage SSbD framework and plan to revise it based on stakeholder feedback. The framework involves establishing key (re)design SSbD principles and assessment of the final innovation, however the applicability of the framework to advanced materials remains to be addressed.

View Article and Find Full Text PDF

Buried interface engineering towards stable zinc anodes for high-performance aqueous zinc-ion batteries.

Sci Bull (Beijing)

December 2024

School of Metallurgy and Environment, Central South University, Changsha 410083, China; Engineering Research Center of the Ministry of Education for Advanced Battery Materials, Central South University, Changsha 410083, China; National Energy Metal Resources and New Materials Key Laboratory, Central South University, Changsha 410083, China. Electronic address:

The dendrite and corrosion issues still remain for zinc anodes. Interface modification of anodes has been widely used for stabilizing zinc anodes. However, it is still quite challenging for such modification to simultaneously suppress zinc dendrites and corrosion issues.

View Article and Find Full Text PDF

Archaeological sites in deltaic regions face increasing environmental threats. This study provides the first assessment of seawater intrusion and land subsidence impacts on archaeological sites in the Nile Delta through hydrochemical investigations, InSAR techniques, and multi-criteria decision analysis of 33 sites. The results reveal that 80.

View Article and Find Full Text PDF

Currently, the main limitations of Pd-coated Nb-TiFe dual-phase alloys include insufficient hydrogen permeability, susceptibility to hydrogen embrittlement (HE), and poor tolerance of HS poisoning. To address these issues, this study proposes a series of improvements. First, a novel NbTiFe alloy composed of a well-aligned Nb-TiFe eutectic was successfully prepared using directional solidification (DS) technology.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!