AI Article Synopsis

  • The study aimed to analyze how different rotary instruments affect the surface roughness of human dentin and its impact on the bond strength of self-etch adhesives.
  • Surface preparation resulted in significant differences in both the dentin's roughness and the micro-tensile bond strength, with cross-cut carbide burs producing the roughest surfaces and tungsten carbide finishing burs yielding the smoothest.
  • High bond strength values were consistently observed for the etch-and-rinse adhesive (OptiBond FL), while self-etch adhesives showed similar bond strength across different rotary instruments.

Article Abstract

Purpose: To characterize the surface roughness of human dentin prepared with different rotary instruments and its influence on the micro-tensile bond strength (microTBS) of self-etch adhesives.

Methods: Dentin surfaces were created from mid-coronal sound dentin in extracted, human third molars. The teeth were ground with high-speed diamond, tungsten carbide finishing, and cross-cut carbide rotary instruments. Morphological changes obtained were investigated with a surface texture analyzer. Two additional specimens from each group were treated and prepared for scanning electron microscopy. Resin composite (Z 100) was bonded to the surfaces using Optibond FL (control), Adper Prompt L-Pop (strong), Clearfil SE Bond (mild), or Clearfil S3 Bond (ultra-mild). Rectangular micro-specimens were prepared using the slow-speed diamond saw and tested in tensile to determine the microTBS. The data were analyzed with one-way analysis of variance and Tukey's HSD test (alpha= 0.05).

Results: Surface preparation resulted in significant differences for surface topography and micro-tensile bond strength (P< 0.001). The cross-cut carbide burs had significantly higher mean roughness readings (SD) for all parameters: Ra [8.6 (1.9) microm], Rq [10.9 (2.2) microm], and Ry [41.1 (2.1) microm], except for the mean Rz [12.1 (3.1) microm] value, which was recorded for diamonds. The other roughness parameters for the diamond rotary instruments were intermediate. Dentin surfaces completed with tungsten carbide finishing burs produced a smoother surface Ra [1.2 (0.5) microm)] Rq ([1.6 (0.6) microm], Ry [6.4 (2.6) microm)] and Rz [1.9 (0.6) microm)]. The etch-and-rinse adhesive (OptiBond FL) yielded high micro-tensile values (58.1-68.3 MPa), irrespective of the rotary instruments used. The micro-tensile bond strength values were comparable for self-etch adhesives (Adper Prompt L-Pop, Clearfil SE Bond, Clearfil S3 Bond) irrespective of the burs used. The microTBS values were significantly higher with tungsten carbide finishing burs and smooth dentin surfaces.

Download full-text PDF

Source

Publication Analysis

Top Keywords

bond strength
16
dentin surfaces
16
rotary instruments
16
clearfil bond
16
micro-tensile bond
12
tungsten carbide
12
carbide finishing
12
bond
8
human dentin
8
cross-cut carbide
8

Similar Publications

Investigate the impact of antimicrobial photodynamic therapy (aPDT) using different photosensitizers (PSs) such as indocyanine green (IG), curcumin (CC), and methylene blue (MB), with or without intracanal application of calcium hydroxide (CH), on the push-out bond strength of glass-fiber posts (GFPs) to intraradicular dentin, the chemical composition of the root substrate, and the sealing of the adhesive interface across different thirds of intraradicular dentin. A total of 112 bovine teeth underwent biomechanical preparation and were divided into eight experimental groups (n = 14 each): Negative control with deionized water; positive control with deionized water + CH; IG group with indocyanine green and infrared laser; IG + CH group; CC group with curcumin and blue LED; CC + CH group; MB group with methylene blue and red laser; and MB + CH group. The push-out bond strength was measured using a universal testing machine (n = 8), and scanning electron microscopy characterized the fracture patterns.

View Article and Find Full Text PDF

Comparing Sectional and Total Dentin Bond Strengths of Three Endodontic Sealers after Using the Single-cone Obturation Technique: An Study.

J Contemp Dent Pract

October 2024

College of Dentistry, Ajman University, Ajman P.O. Box 346, United Arab Emirates; Department of Endodontic, Faculty of Dentistry, Mansoura University, Egypt, Orcid: https://orcid.org/0000-0003-3391-5306.

Aim: This study aimed to investigate and compare the total and sectional bond strengths of three endodontic sealers when used with the single-cone obturation technique.

Materials And Methods: Forty-five human maxillary central incisors were prepared and divided into three groups according to the type of endodontic sealer: Group I (Gutta-percha/AH Plus Jet), group II (Gutta-percha/GuttaFlow 2), and group III (RealSeal/RealSeal SE). All canals were filled with the single-cone technique.

View Article and Find Full Text PDF

Effect of Mushroom, Ozone Gas, and Their Combination as Pretreatment Materials on the Bond Strength of Resin Composite to Dentin.

J Contemp Dent Pract

October 2024

Department of Dental Biomaterials, Faculty of Dental Medicine for Girls, Al-Azhar University, Cairo, Egypt, Orcid: https://orcid.org/0000-0002-3420-4146.

Aim: To assess the effect of mushrooms, ozone gas, and their combination as cavity disinfectants on the bonding strength of composite to dentin.

Materials And Methods: The study was conducted on 40 sound premolar teeth randomly divided into four groups. Group I: control group, Group II: mushroom group, Group III: Ozone group, and Group IV: mushroom + ozone gas (combination) group.

View Article and Find Full Text PDF

Background/purpose: The efficacy of riboflavin-ultraviolet-A (RF-UVA) treatment in crosslinking collagen and improving dentin bonding has been proven. However, biodegradation of the hybrid layer may compromise the bonding. The purpose of this study was to evaluate different RF-UVA treatments regarding their ability to preserve dentin bonding from enzymatic digestion.

View Article and Find Full Text PDF

Purpose: To evaluate the shear bond strength (SBS) of stereolithography (SLA), digital light processing (DLP) manufactured, and computer numerical control (CNC) milled zirconia to veneering ceramic.

Materials And Methods: Rectangular shaped zirconia substrates (10 × 5 × 5 mm) were manufactured through SLA, DLP, and CNC technology separately. Their surface roughness was measured and the surface topography was analyzed by atomic force microscope (AFM).