Determination of arsenic leaching from glazed and non-glazed Turkish traditional earthenware.

Sci Total Environ

Department of Chemistry, Faculty of Science, University of Ege, 35100 Bornova, İzmir, Turkey.

Published: July 2011

Glazed and non-glazed earthenware is traditionally and widely used in Turkey and most of the Mediterranean and the Middle East countries for cooking and conservation of foodstuff. Acid-leaching tests have been carried out to determine whether the use of glazed and non-glazed earthenware may constitute a human health hazard risk to the consumers. Earthenware was leached with 4% acetic acid and 1% citric acid solutions, and arsenic in the leachates was measured using hydride generation atomic absorption spectrometry. Arsenic concentrations in the leach solution of non-glazed potteries varied from 30.9 to 800 μg L⁻¹, while the glazed potteries varied generally from below the limit of detection (0.5 μg L⁻¹) to 30.6 μg L⁻¹, but in one poorly glazed series it reached to 110 μg L⁻¹. Therefore, the risk of arsenic poisoning by poorly glazed and non-glazed potteries is high enough to be of concern. It appears that this is the first study reporting arsenic release from earthenware into food.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.scitotenv.2011.04.027DOI Listing

Publication Analysis

Top Keywords

glazed non-glazed
16
μg l⁻¹
16
non-glazed earthenware
8
non-glazed potteries
8
potteries varied
8
l⁻¹ glazed
8
glazed
6
non-glazed
5
earthenware
5
determination arsenic
4

Similar Publications

Aging of monolithic zirconia dental prostheses: Protocol for a 5-year prospective clinical study using e analyses.

Contemp Clin Trials Commun

December 2016

Dental Biomaterials Research Unit (d-BRU) and Department of Fixed Prosthodontics, Institute of Dentistry, University of Liège (ULg) and University of Liège Hospital (CHU), 45 Quai G. Kurth, Liège, 4020, Belgium.

Background: Recent introduction of computer-aided design/computer-aided manufacturing (CAD/CAM) monolithic zirconia dental prostheses raises the issue of material low thermal degradation (LTD), a well-known problem with zirconia hip prostheses. This phenomenon could be accentuated by masticatory mechanical stress. Until now zirconia LTD process has only been studied .

View Article and Find Full Text PDF

Aim: The objective of this study was to evaluate the effect of the polishing technique and glazing on the porosity of the dental resins.

Material And Methods: The studied resins were: Castapress/Vertex, Prothyl Hot/Zermack, Rapid Simplified/Vertex, Duracryl Plus/Spofa Dental, Vertex-Soft/Vertex, Superacryl Plus/Spofa Dental. Thirty specimens, five for every resin, of 50/25/2 cm in size were done.

View Article and Find Full Text PDF

Determination of arsenic leaching from glazed and non-glazed Turkish traditional earthenware.

Sci Total Environ

July 2011

Department of Chemistry, Faculty of Science, University of Ege, 35100 Bornova, İzmir, Turkey.

Glazed and non-glazed earthenware is traditionally and widely used in Turkey and most of the Mediterranean and the Middle East countries for cooking and conservation of foodstuff. Acid-leaching tests have been carried out to determine whether the use of glazed and non-glazed earthenware may constitute a human health hazard risk to the consumers. Earthenware was leached with 4% acetic acid and 1% citric acid solutions, and arsenic in the leachates was measured using hydride generation atomic absorption spectrometry.

View Article and Find Full Text PDF

Purpose: Zirconia-based ceramics offer strong restorations in dentistry, but the adhesive bond strength of resin cements to such ceramics is not optimal. This study evaluated the bond strength of silane/adhesive/resin cement and zirconia primer/resin cement combinations on non-glazed and glazed zirconia surfaces before and after aging.

Materials And Methods: Disk-shaped zirconia ceramic specimens (diameter: 8 mm; thickness: 2 mm) (N = 80, n = 10 per group) were randomly divided into 2 groups.

View Article and Find Full Text PDF

Objective: The aim of this study was to evaluate the bond strength between metal brackets and non-glazed ceramic with three different surface treatment methods.

Materials And Methods: Forty-two non-glazed ceramic disks were assigned into three groups. Group I and II specimens were etched with 9.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!