Mechanical reinforcement of nanoparticle thin films using atomic layer deposition.

ACS Nano

Department of Chemical and Biomolecular Engineering, University of Pennsylvania, Philadelphia, Pennsylvania 19104, United States.

Published: June 2011

Thin films composed of nanoparticles exhibit synergistic properties, making them useful for numerous advanced applications. Nanoparticle thin films (NTFs), however, have a very low resistance to mechanical loading and abrasion, presenting a major bottleneck to their widespread use and commercialization. High-temperature sintering has been shown to improve the mechanical durability of NTFs on inorganic substrates; however, these high-temperature processes are not amenable to organic substrates. In this study, we demonstrate that the mechanical durability of TiO(2)/SiO(2) nanoparticle layer-by-layer (LbL) films on glass and polycarbonate substrates can be drastically improved using atomic layer deposition (ALD) at a relatively low temperature. The structure and physical properties of ALD-treated TiO(2)/SiO(2) nanoparticle LbL films are studied using spectroscopic ellipsometry, UV-vis spectroscopy, contact angle measurements, and nanoindentation. The composition of TiO(2)/SiO(2) LbL films as a function of ALD-cycle number is determined through solution ellipsometry, enabling the determination of the characteristic pore size of nanoparticle thin films. Mechanical durability is also investigated by abrasion tests, showing that the robustness of ALD-treated nanoparticle films is comparable to that of thermally calcined films. More importantly, ALD-treated nanoparticle films retain the original functionality of the TiO(2)/SiO(2) LbL films, such as superhydrophilicity and antireflection properties, demonstrating the utility of ALD as a reinforcement method for nanoparticle thin films.

Download full-text PDF

Source
http://dx.doi.org/10.1021/nn201167jDOI Listing

Publication Analysis

Top Keywords

thin films
20
nanoparticle thin
16
lbl films
16
films
12
mechanical durability
12
nanoparticle
8
atomic layer
8
layer deposition
8
tio2/sio2 nanoparticle
8
tio2/sio2 lbl
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!