This study evaluated the bonding characteristics to ground and unground enamel obtained with different strategies. For this purpose, 24 sound third-molars were bisected mesiodistally to obtain tooth halves. A flat enamel area was delimited in the tooth sections, which were randomly distributed into 8 groups (n=6), according to the enamel condition (ground and unground) and adhesive system (Adper Single Bond 2 - SB2; Adper Prompt L-Pop - PLP; Adper Prompt - AD; Clearfil SE Bond - SE). Each system was applied according manufacturers' instructions and a 6-mm-high resin composite "crown" was incrementally built up on bonded surfaces. Hourglass-shaped specimens with 0.8 mm(2) cross-section were produced. Microtensile bond strength (μTBS) was recorded and the failure patterns were classified. Results were analyzed by two-way ANOVA and Tukey's test (α=0.05). There were no statistically significant differences among the μTBS values of SB2, PLP and AD (p>0.05). SE values were significantly lower (p0.05). There was prevalence of cohesive failure within enamel, adhesive system and resin composite for SB2. The self-etch systems produced higher incidence of cohesive failures in the adhesive system. Enamel condition did not determine significant differences on bonding characteristics for the same bonding system. In conclusion, the bonding systems evaluated in this study resulted in specific μTBS and failure patterns due to the particular interaction with enamel.

Download full-text PDF

Source
http://dx.doi.org/10.1590/s0103-64402011000200006DOI Listing

Publication Analysis

Top Keywords

bonding characteristics
12
adhesive system
12
microtensile bond
8
bond strength
8
unground enamel
8
ground unground
8
enamel condition
8
adper prompt
8
resin composite
8
failure patterns
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!