The ability of a restorative material to withstand fracture is of crucial importance especially in stress-bearing area. Therefore, the study aims to analyse the fracture toughness of a large number of dental restorative materials categories. The fracture toughness (K(IC)) of 69 restorative materials belonging to ten materials categories-micro-hybrid, nanofilled, microfilled, packable, ormocer-based, and flowable resin-based composites (RBC), compomers and flowable compomers, as well as glass ionomer cements (GIC) and resin-modified GIC was measured by means of the single-edge notched-beam method after storing the samples (n = 8) for 24 h in distilled water. Data were analyzed with the one-way analysis of variance (ANOVA) followed by the Tukey's test and partial eta-squared statistics (p < 0.05). Large variations between the tested materials within a material category were found. The lowest fracture toughness was reached in the GIC group, followed by the microfilled RBCs, resin-modified GIC, and flowable compomers, which do not differ significantly among each other as a material group. The ormocer-based, packable, and micro-hybrid RBCs performed statistically similar, reaching the highest fracture toughness values. Between the two categories of flowables-composites and compomers-no differences were measured. The correlation between K(IC) and filler volume (0.34) and respective filler weight (0.40) was low. K(IC) increased with the volume fraction of fillers until a critical value of 57%, following with a plateau, with constant values until ca. 65% volume fraction. Above this value, K(IC) decreased slightly. Due to the very large variability of the fracture toughness within a material type, the selection of a suitable restorative material should have not been done with respect to a specific material category, especially in stress-bearing areas, but by considering the individual measured material properties.

Download full-text PDF

Source
http://dx.doi.org/10.1007/s00784-011-0525-zDOI Listing

Publication Analysis

Top Keywords

fracture toughness
12
restorative materials
12
dental restorative
8
fracture
4
toughness dental
4
restorative
4
materials
4
materials ability
4
ability restorative
4
restorative material
4

Similar Publications

Low fracture toughness, low-temperature degradation (LTD) susceptibility, and inadequate soft tissue integration greatly limit the application of zirconia ceramic abutment. Integrating the "surface" of hard all-ceramic materials into the gingival soft tissue and simultaneously promoting the "inner" LTD resistance and fracture toughness is challenging. Composite ceramics are effective in improving the comprehensive properties of materials.

View Article and Find Full Text PDF

Fracture resistances of heat-treated nickel-titanium files used for minimally invasive instrumentation.

BMC Oral Health

January 2025

Department of Conservative Dentistry, School of Dentistry, Dental Research Institute, Dental and Life Science Institute, Pusan National University, Yangsan, Korea.

Background: This study compared the torsional resistance, bending stiffness, and cyclic fatigue resistances of different heat-treated NiTi files for minimally invasive instrumentation.

Methods: TruNatomy (TN) and EndoRoad (ER) file systems were compared with ProTaper Gold (PG). Torsional load, distortion angle, and bending stiffness were assessed using a custom device AEndoS, and toughness was calculated using the torsional data.

View Article and Find Full Text PDF

Robust Mechanically Interlocked Network Ionogels.

Angew Chem Int Ed Engl

January 2025

Shanghai Jiao Tong University, School of Chemistry and Chemical Engineering, 800 Dongchuan Road, 200240, Shanghai, CHINA.

Ionogels have attracted considerable attention as versatile materials due to their unique ionic conductivity and thermal stability. However, relatively weak mechanical performance of many existing ionogels has hindered their broader application. Herein, we develop robust, tough, and impact-resistant mechanically interlocked network ionogels (IGMINs) by incorporating ion liquids with mechanical bonds that can dissipate energy while maintain structural stability.

View Article and Find Full Text PDF

Fiber-based artificial muscles are soft actuators used to mimic the movement of human muscles. However, using high modulus oxide ceramics to fabricate artificial muscles with high energy and power is a challenge as they are prone to brittle fracture during torsion. Here, a ceramic metallization strategy is reported that solves the problem of low torsion and low ductility of alumina (AlO) ceramics by chemical plating a thin copper layer on alumina filaments.

View Article and Find Full Text PDF

Nanocomposites of epoxy with FeO featuring dynamic disulfide bonds were fabricated. To facilitate the dispersion of FeO nanoparticles, we synthesized poly(ε-caprolactone)-grafted FeO nanoparticles, which were then incorporated into epoxy to generate robust interfacial interactions between epoxy and the inorganic nanoparticles. Through this approach, a fine dispersion of the inorganic nanoparticles in the epoxy matrix was successfully obtained.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!