The effect of holding time on nanoindentation measurements of creep in bone.

J Biomech

Tissue Mechanics Laboratory, Department of Aerospace and Mechanical Engineering, University of Notre Dame, Notre Dame, IN 46556, USA.

Published: April 2011

Viscoelasticity may affect both the elastic and fracture characteristics of bone. Nanoindentation can be used to measure the creep behavior of bone by fitting the depth vs. time data at constant load to rheological models. However, the creep data may be influenced by latent effects arising during the loading phase of indentation. As such, the loading protocol, particularly the holding time, may affect the measured creep time constants. To characterize the effect of holding time on the measures, four cortical bone samples were prepared from four bovine femora and subjected to nanoindentation to measure the creep behavior. The creep time constants were found by fitting the indentation depth vs. time curve to three different rheological models: the standard linear solid, Burgers model, and a two-dashpot Kelvin model. All three models provided good fits to the data, which were relatively insensitive to the initial parameter estimates. The calculated creep time constants increased monotonically with increasing holding time for all three models. However, the relative differences between measurements within a single osteon, within a single sample, and between samples were maintained for creep holding times over 16s. Hence, while the creep time constants measured by nanoindentation with hold times up to 30s may not provide accurate property measurements, comparisons between samples are valid if all are assessed at the same holding time. Considering the long-term viscosity of bone tissue, Burgers model provided the best performance in terms of stability and goodness of fit, and is recommended for future studies.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC3065521PMC
http://dx.doi.org/10.1016/j.jbiomech.2011.01.039DOI Listing

Publication Analysis

Top Keywords

holding time
20
creep time
16
time constants
16
time
10
creep
9
nanoindentation measure
8
measure creep
8
creep behavior
8
depth time
8
rheological models
8

Similar Publications

Value of multi-parameter I-MIBG scintigraphy in the differential diagnosis of Parkinson's disease.

EJNMMI Res

January 2025

Department of Nuclear Medicine, Beijing Friendship Hospital, Capital Medical University, 95 Yong'an Road, Xicheng District, Beijing, China.

Background: I-MIBG scintigraphy plays a significant role in diagnosing Parkinson's disease (PD), with most studies primarily targeting cardiac uptake and relying on traditional ratio-based parameters for assessment. However, due to variations in scanning conditions and image processing methodologies, the clinical utility of different parameters remains a subject of debate. This study aims to evaluate the diagnostic accuracy of multi-parameter I-3-Iodobenzylguanidine (MIBG) scintigraphy and to identify the most reliable metrics for distinguishing PD from Parkinson-plus syndromes.

View Article and Find Full Text PDF

A nearly ubiquitous negative relationship between taxonomic richness and mean range-size (average area of taxa) is observed across space. However, the complexity of the mechanism limits its applicability for conservation or range prediction. We explore whether the relationship holds over time, and whether plant speciation, environmental heterogeneity, or plant interactions are major factors of the relationship within northeast Siberia and Alaska.

View Article and Find Full Text PDF

Predicting disease trajectories in patients with major depressive disorder (MDD) can allow designing personalized therapeutic strategies. In this study, we aimed to show that measuring patients' plasticity - that is the susceptibility to modify the mental state - identifies at baseline who will recover, anticipating the time to transition to wellbeing. We conducted a secondary analysis in two randomized clinical trials, STAR*D and CO-MED.

View Article and Find Full Text PDF

Climate change is a spatial and temporarily non-uniform phenomenon that requires understanding its evolution to better evaluate its potential societal and economic impact. The value added of this paper lies in introducing a quantitative methodology grounded in the trend analysis of temperature distribution quantiles to analyze climate change heterogeneity (CCH). By converting these quantiles into time series objects, the methodology empowers the definition and measurement of various relevant concepts in climate change analysis (warming, warming typology, warming amplification and warming acceleration) in a straightforward and robust testable linear regression format.

View Article and Find Full Text PDF

The 2024 Zurich perfluorinated compounds (PFCs) summit reiterated the urgent need for non-selective analytical approaches for PFC detection. 19F NMR holds great potential, however, sensitivity limitations lead to long analysis times and/or the possibility of not detecting low concentration species. Steady State Free Precession (SSFP) NMR collects the signal in a steady state regime, allowing 100's of acquisitions in the timespan of a single traditional NMR scan.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!