Using the push-out test, this study evaluated the bond strength of the composite resin Z250 (3M/ESPE) photoactivated with the XL2500 (3M/ESPE) quartz-tungsten-halogen light-curing unit with different curing protocols: soft-start (150 mW/cm² for 2 s (S2), 3 s (S3), 5 s (S5), 10 s (S10) or 15 s (S15), followed by 700 mW/cm² for 15 s; pulse-delay (150 mW/cm² for 2 s (P2), 3 s (P3), 5 s (P5), 10 s (P10) or 15 s (P15), with a 1-min delay, followed by 700 mW/cm² for 15 s. After storage at 37°C ± 1 for 24 h ± 1, the specimens were ground, polished and subjected to a push-out test in a universal test machine (Instron) with a cell load of 500 N at a crosshead speed of 0.5 mm/min. The data were analyzed statistically by ANOVA and Tukey's test at 5% significance level. There were no statistically significant differences (p>0.05) among the groups photoactivated using the soft-start mode. For the pulse-delay mode, P5 promoted the highest bond strength (p<0.05). Groups photoactivated with the pulse-delay mode (except for P2 and P15) presented significantly higher bond strength than those photoactivated with the soft-start. It may be concluded that the influence of initial exposure time was curing method-dependent, with the best results obtained using the pulse-delay method with 5 s in the first photoactivation cycle.

Download full-text PDF

Source
http://dx.doi.org/10.1590/s0103-64402010000300008DOI Listing

Publication Analysis

Top Keywords

bond strength
12
push-out test
8
150 mw/cm²
8
700 mw/cm²
8
photoactivation techniques
4
techniques bond
4
strength dental
4
dental composite
4
composite push-out
4
test
4

Similar Publications

Shear bond strength and ARI scores of metal brackets to glazed glass ceramics and zirconia: an in vitro study investigating surface treatment protocols.

BMC Oral Health

December 2024

Faculty of Dentistry, Innovative Dental Materials and Interfaces Research Unit (URB2i), UR 4462, Paris Cité University, 1 rue Maurice Arnoux, Montrouge, 92120, France.

Objective: To evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) scores of metal brackets to glazed lithium disilicate reinforced glass-ceramics and zirconia according to various surface treatment protocols.

Methods: A total of 240 lithium disilicate ceramic (LD) and 240 zirconia (Zr) blocks were randomly divided according to sandblasting, hydrofluoric acid (HF) etching, universal primer use, and the adhesive system applied. A maxillary canine metal bracket was bonded to each sample with resin cement (Transbond XT, TXT).

View Article and Find Full Text PDF

This study investigated the effects of resin composites (RCs) containing surface pre-reacted glass ionomer (S-PRG) filler on the dentin microtensile bond strength (μTBS) of HEMA-free and HEMA-containing universal adhesives (UAs). Water sorption (WS) and solubility (SL), degree of conversion (DC), and ion release were measured. The UAs BeautiBond Xtreme (BBX; 0% HEMA), Modified Adhesive-1 (E-BBX1; 5% HEMA), Modified Adhesive-2 (E-BBX2; 10% HEMA), and two 2-step self-etch adhesives (2-SEAs): FL-BOND II (FBII; with S-PRG filler) and silica-containing adhesive (E-FBII) were used.

View Article and Find Full Text PDF

Bond strength between repair and restorative materials is crucial for endodontic success. This study assessed the effects of the following final irrigation solutions on the bond strength of mineral trioxide aggregate (MTA) to a bulk-fill composite: (1) 17% Ethylenediamine tetraacetic acid (EDTA); (2) 2% Chlorhexidine (CHX); (3) 0.2% chitosan; (4) 0.

View Article and Find Full Text PDF

The aim of the study is to assess the impact of mechanical surface treatments on the shear bond strength (SBS) of orthodontic brackets bonded to three-dimensional (3D) printed and milled CAD/CAM provisional materials. Sixty cylindrical samples were fabricated for each provisional material. Samples were treated with one of the following surface treatments: aluminum oxide airborne particle abrasion, diamond bur rotary instrument roughening, and phosphoric acid etching (control).

View Article and Find Full Text PDF

Adhesion within endodontic obturation material and root canal walls improves the efficacy of the endodontic treatment by establishing a barrier that inhibits reinfection and entombs residual bacteria. This study evaluates the push-out bond strength (POBS) of calcium silicate sealers compared to an epoxy-resin-based sealer. A total of 36 extracted mono-radicular teeth were prepared with Pro Taper Ultimate and irrigated with 5.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!