Fracture surface analysis to understand the failure mechanisms of collagen degraded bone.

J Bone Miner Metab

Samuel Lunenfeld Research Institute, Mount Sinai Hospital, 600 University Avenue, Room 840, Toronto, ON M5G 1X5, Canada.

Published: May 2011

Fracture surface analysis is a powerful technique to investigate bone failure mechanisms. Previously, emu tibiae were endocortically treated with 1 M potassium hydroxide (KOH) solution for 14 days. This treatment caused in situ collagen degradation rather than removal, with no differences in geometrical parameters, but with significant changes in mechanical properties. KOH-treated tibiae showed significant decreases in failure stress and increased failure strain and toughness. The fracture surfaces of untreated and 14-day KOH-treated failed specimens were examined to further identify differences in the failure process to explain the previously observed increase in toughness. Areas of 'tension,' 'compression,' and 'transition' were identified using digital images of the fracture surfaces. Within these areas, the degree of 'roughness' and 'smoothness' was identified and estimated, using an optical profiler and SEM images. The fracture surfaces of 14-day KOH-treated bones showed a significantly higher 'roughness' compared to untreated bones. Furthermore, additional toughening mechanisms, which are important features for dissipating energy during the failure process, were observed in KOH-treated samples, but were absent in untreated samples. These results indicate that the significant increase in toughness of KOH treated bones is the result of structural alterations that enhance the ability of the microstructure to dissipate energy during the failure process, thereby slowing crack propagation. Fracture surface analysis has helped explain why KOH-treated bones have increased toughness compared to untreated bones, namely via toughening mechanisms on the compressive failure side.

Download full-text PDF

Source
http://dx.doi.org/10.1007/s00774-010-0233-9DOI Listing

Publication Analysis

Top Keywords

fracture surface
12
surface analysis
12
fracture surfaces
12
failure process
12
failure
8
failure mechanisms
8
14-day koh-treated
8
increase toughness
8
images fracture
8
koh-treated bones
8

Similar Publications

Mechanochemistry and mechanocatalysis are gaining increasing attention as environmentally friendly chemical processes because of their solvent-free nature and scalability. Significant effort has been devoted for studying continuum-scale phenomena in mechanochemistry, such as temperature and pressure gradients, but the atomic-scale mechanisms remain relatively unexplored. In this work, we focus on the mechanochemical reduction of MoO as a case study.

View Article and Find Full Text PDF

Objectives: Previous studies reported various methods of measuring fracture toughness of dental ceramics. The objectives of this study were to compare different methods and to validate fractal analysis to estimate fracture toughness for a polycrystalline dental ceramic.

Methods: Bar-shaped specimens were prepared from 3 mol% yttria-stabilized tetragonal polycrystalline (3Y-TZP) ceramic.

View Article and Find Full Text PDF

Mechanical properties of a polylactic 3D-printed interim crown after thermocycling.

PLoS One

January 2025

Department of Advanced General Dentistry, College of Dentistry, Yonsei University, Seoul, Korea.

Polylactic acid (PLA) has garnered attention for use in interim dental restorations due to its biocompatibility, biodegradability, low cost, ease of fabrication, and moderate strength. However, its performance under intraoral conditions, particularly under heat and moisture, remains underexplored. This study evaluated the mechanical properties of PLA interim crowns compared with those of polymethylmethacrylate (PMMA) and bisphenol crowns under simulated intraoral conditions with thermocycling.

View Article and Find Full Text PDF

Joint endoprosthetics is one of the most successful surgical-orthopedic procedures worldwide, enabling pain reduction and complete restoration of mobility. In the Federal Republic of Germany, around 400,000 joint endoprostheses, hip and knee joints are currently implanted every year ( https://www.eprd.

View Article and Find Full Text PDF

Fiber-reinforced polymer composites are subjected to harsh environmental conditions over the course of their designed lifespan. Studying the aging process of fiber-reinforced polymer composites exposed to boiling water is critical for improving their durability. This study uses a hand lay-up technique to fabricate composites from glass fiber, bamboo fiber, nanoclay, and epoxy.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!