We prepared ultrafine Fe-Pt alloy nanoparticle colloids by UV laser solution photolysis (KrF excimer laser of 248 nm wavelength) using precursors of methanol solutions into which iron and platinum complexes were dissolved together with PVP dispersant to prevent aggregations. From TEM observations, the Fe-Pt nanoparticles were found to be composed of disordered FCC A1 phase with average diameters of 0.5-3 nm regardless of the preparation conditions. Higher iron compositions of nanoparticles require irradiations of higher laser pulse energies typically more than 350 mJ, which is considered to be due to the difficulty in dissociation of Fe(III) acetylacetonate compared with Pt(II) acetylacetonate. Au colloid preparation by the same method was also attempted, resulting in Au nanoparticle colloids with over 10 times larger diameters than the Fe-Pt nanoparticles and UV-visible absorption peaks around 530 nm that originate from the surface plasmon resonance. Differences between the Fe-Pt and Au nanoparticles prepared by the KrF excimer laser solution photolysis are also discussed.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC2894087PMC
http://dx.doi.org/10.1007/s11671-009-9281-2DOI Listing

Publication Analysis

Top Keywords

nanoparticle colloids
12
krf excimer
12
excimer laser
12
laser solution
12
solution photolysis
12
fe-pt nanoparticles
12
ultrafine fe-pt
8
fe-pt alloy
8
alloy nanoparticle
8
fe-pt
5

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!