The aim of this study was to evaluate the effects of three desensitizing agents on the shear bond strengths of four different bonding agents used to bond composite resin to dentin. A total of 160 extracted human molars were sectioned parallel to the occlusal plane under water cooling, polished and randomly divided into 4 groups of 40. Each group was treated with a different desensitizing agent (Tooth Mousse, Ultra-EZ, Cervitec Plus), except for an untreated control group. Each group was then randomly subdivided into 4 groups of 10, and a different dentin bonding agent (XP Bond, AdheSE, Adper Prompt L-pop, GBond) was applied to each group in order to bond the specimens to a resin composite (Gradia Direct) built up using a plastic apparatus. A Universal Testing Machine was used to measure the shear bond strength of each specimen. Statistical analysis was performed using one-way ANOVA and Tukey's tests. With the exception of the Control/AdheSE and Ultra-EZ/XP Bond groups, no statistically significant differences were found in the shear bond strength values of the groups tested. These findings suggest that the use of different desensitizing agents does not affect the shear bond strength of various adhesive systems used to bond resin composite to dentin.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1016/j.jmbbm.2010.03.003 | DOI Listing |
J Contemp Dent Pract
October 2024
Department of Dental Biomaterials, Faculty of Dental Medicine for Girls, Al-Azhar University, Cairo, Egypt, Orcid: https://orcid.org/0000-0002-3420-4146.
Aim: To assess the effect of mushrooms, ozone gas, and their combination as cavity disinfectants on the bonding strength of composite to dentin.
Materials And Methods: The study was conducted on 40 sound premolar teeth randomly divided into four groups. Group I: control group, Group II: mushroom group, Group III: Ozone group, and Group IV: mushroom + ozone gas (combination) group.
J Prosthodont
January 2025
Department of Prosthodontics, Shanghai Ninth People's Hospital, Shanghai Jiao Tong University School of Medicine; College of Stomatology, Shanghai Jiao Tong University; National Center for Stomatology; National Clinical Research Center for Oral Diseases; Shanghai Key Laboratory of Stomatology; Shanghai Research Institute of Stomatology, Shanghai, PR China.
Purpose: To evaluate the shear bond strength (SBS) of stereolithography (SLA), digital light processing (DLP) manufactured, and computer numerical control (CNC) milled zirconia to veneering ceramic.
Materials And Methods: Rectangular shaped zirconia substrates (10 × 5 × 5 mm) were manufactured through SLA, DLP, and CNC technology separately. Their surface roughness was measured and the surface topography was analyzed by atomic force microscope (AFM).
Int J Dent
January 2025
Department of Orthodontics, School of Dentistry, Mashhad University of Medical Sciences, Mashhad, Iran.
This research aimed to assess the shear bond strength (SBS) of metal brackets bonded to composite veneers using different surface preparations. One-hundred composite disks were divided into 10 different groups whereby each group combines a surface preparation (roughening or no roughening), etching agent (37% phosphoric or 9.5% hydrofluoric acid), adhesive protocol (self-etch or total-etch), and bonding agent (with or without G-Premio Bond).
View Article and Find Full Text PDFMaterials (Basel)
January 2025
Department of Preventive Dentistry, Periodontology and Cariology, University Medical Center Göttingen, 37075 Göttingen, Germany.
To investigate the effect of different sandblasting settings on the shear bond strength (SBS) in the repair of resin composite, specimens (resin composite, enamel, and dentin; each group = 16) were sandblasted by varying the parameters of air pressure (0.2/0.3/0.
View Article and Find Full Text PDFMaterials (Basel)
January 2025
Division of Biomaterials, School of Dentistry, University of Alabama at Birmingham, Birmingham, AL 35209, USA.
Two 3D-printed crown materials (Crown and Ceramic Crown) were examined to determine the best surface treatment and primers for bonding. Discs of the two materials were printed and mounted with their "intaglio" surfaces untouched. Half the specimens from each group were sandblasted with 50 µm alumina.