Characterization of indentation response and stiffness reduction of bone using a continuum damage model.

J Mech Behav Biomed Mater

Department of Aerospace and Mechanical Engineering, University of Notre Dame, Notre Dame, IN 46556, USA.

Published: February 2010

Indentation tests can be used to characterize the mechanical properties of bone at small load/length scales offering the possibility of utilizing very small test specimens, which can be excised using minimally-invasive procedures. In addition, the need for mechanical property data from bone may be a requirement for fundamental multi-scale experiments, changes in nano- and micro-mechanical properties (e.g., as affected by changes in bone mineral density) due to drug therapies, and/or the development of computational models. Load vs. indentation depth data, however, is more complex than those obtained from typical macro-scale experiments, primarily due to the mixed state of stress, and thus interpretation of the data and extraction of mechanical properties is more challenging. Previous studies have shown that cortical bone exhibits a visco-elastic response combined with permanent deformation during indentation tests, and that the load vs. indentation depth response can be simulated using a visco-elastic/plastic material model. The model successfully captures the loading and creep displacement behavior, however, it does not adequately reproduce the unloading response near the end of the unloading cycle, where a pronounced decrease in contact stiffness is observed. It is proposed that the stiffness reduction observed in bone results from an increase in damage; therefore, a plastic-damage model was investigated and shown capable of simulating a typical bone indentation response through an axisymmetric finite element simulation. The plastic-damage model was able to reproduce the full indentation response, especially the reduced stiffness behavior exhibited during the latter stages of unloading. The results suggest that the plastic-damage model is suitable for describing the complex indentation response of bone and may provide further insight into the relationship between model parameters and mechanical/physical properties.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC2818081PMC
http://dx.doi.org/10.1016/j.jmbbm.2009.08.001DOI Listing

Publication Analysis

Top Keywords

indentation response
16
plastic-damage model
12
stiffness reduction
8
bone
8
indentation tests
8
mechanical properties
8
load indentation
8
indentation depth
8
response
7
model
7

Similar Publications

This manuscript highlights the behavior of biodegradable polymers (PLA and HD PLA Green) coated with two distinct bronze alloy powders, Metco 51F-NS (Cu 9.5Al 1.2Fe) and Metco 445 (Cu 9.

View Article and Find Full Text PDF

Thermal- and Rate-Regulated Fast Switchable Adhesion within Glass Transition Zone of an Epoxy Polymer.

Langmuir

January 2025

Institute of Advanced Manufacturing Technology, Hefei Institutes of Physical Science, Chinese Academy of Sciences, Changzhou 213164, People's Republic of China.

Thermoresponsive shape memory polymer (SMP) adhesives have demonstrated a high adhesion strength and large switching ratios on different substrates. However, a long response time to switch adhesion on or off is generally encountered. This study provides a fast adhesion switching method based on the temperature and rate dependence of adhesion within the glass-transition zone of an epoxy polymer.

View Article and Find Full Text PDF

This research demonstrates a systematic curve fitting approach for acquiring parametric values of hyperelastic constitutive models for both healthy and enzymatically mediated degenerated cartilage to facilitate finite element modeling of cartilage. Several widely used phenomenological hyperelastic constitutive models were tested to adequately capture the changes in cartilage mechanics that vary with the differential/unequal abundance of matrix metalloproteinases (MMPs). Trauma and physiological conditions result in an increased production of collagenases (MMP-1) and gelatinases (MMP-9), which impacts the load-bearing ability of cartilage by significantly deteriorating its extracellular matrix (ECM).

View Article and Find Full Text PDF

Monitoring defects in plates using topological acoustic sensing and sideband peak counting.

Ultrasonics

January 2025

New Frontiers of Sound Science and Technology Center, University of Arizona, Tucson, AZ 85721, USA; Department of Materials Science and Engineering, University of Arizona, Tucson, AZ 85721, USA.

We demonstrate an integrated non-destructive inspection methodology that employs the nonlinear ultrasonics-based sideband peak counting (SPC) technique in conjunction with topological acoustics (TA) sensing to comprehensively characterize the acoustic response of steel plates that contain differing levels of damage. By combining the SPC technique and TA, increased sensitivity to defect/damage detection as well as the ability to spatially resolve the presence of defects was successfully established. Towards this end, using a Rockwell hardness indenter, steel plates were subject to one, three and five centrally located indentations respectively.

View Article and Find Full Text PDF

Response of Differently Structured Dental Polymer-Based Composites to Increasingly Aggressive Aging Conditions.

Nanomaterials (Basel)

January 2025

Department of Conservative Dentistry, University Hospital, Ludwig-Maximilians-University, Goethestr. 70, D-80336 Munich, Germany.

Objective: It is hypothesized that the way nano- and micro-hybrid polymer-based composites are structured and cured impacts the way they respond to aging.

Material And Methods: A polymer-ceramic interpenetrating network composite (Vita Enamic/VE), an industrially polymerized (Brillinat CriosST/BC), and an in situ light-cured composite with discrete inorganic fillers (Admira Fusion5/AF5) were selected. Specimens (308) were either cut from CAD/CAM blocks (VE/BC) or condensed and cured in white polyoxymethylene molds (AF5) and subjected to four different aging conditions ( = 22): (a) 24 h storage in distilled water at 37 °C; (b) 24 h storage in distilled water at 37 °C followed by thermal cycling for 10,000 cycles 5/55 °C (TC); (c) TC followed by storage in a 75% ethanol-water solution; and (d) TC followed by a 3-week demineralization/remineralization cycling.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!