Transparent BaTiO(3):Eu(3+) films were prepared via a sol-gel method and dip-coating technique, using barium acetate, titanium butoxide, and polyvinylpyrrolidone (PVP) as modifier viscosity. BaTiO(3):Eu(3+) films ~500 nm thick, crystallized after thermal treatment at 700 masculineC. The powders revealed spherical and rod shape morphology. The optical quality of films showed a predominant band at 615 nm under 250 nm excitation. A preliminary luminescent test provided the properties of the Eu(3+) doped BaTiO(3).

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC2769136PMC
http://dx.doi.org/10.3390/ijms10094088DOI Listing

Publication Analysis

Top Keywords

batio3eu3+ films
8
eu-doped batio₃powder
4
batio₃powder film
4
film sol-gel
4
sol-gel process
4
process polyvinylpyrrolidone
4
polyvinylpyrrolidone additive
4
additive transparent
4
transparent batio3eu3+
4
films prepared
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!