Background, Aim, And Scope: The first step in the restoration of a medieval stained glass window is the evaluation of its degree of degradation. This implies the study of the chemical composition of the stained glass as well as the new mineral phases developed on its surface (patinas). Patinas are clearly related to glass composition, time, environmental conditions, microenvironments developed in local zones, bioactivity, physical and chemical factors, etc. This study was carried out on patinas developed in selected Na-rich stained glass of the Santa Maria de Pedralbes Monastery (Barcelona, Spain). The location of this monument in the city (about 5 km from the shoreline and close to the Collserola hill flank) helped to determine the environmental conditions in which patinas developed. The aim of our study was to characterize the patinas formed on the surface of the selected glass of this monastery in order to understand the role of the chemical composition of the original glass (Na-rich) as well as the environmental conditions in which they developed.

Materials And Methods: Powdered samples of two different color-type patinas (ochre-orange and brownish) were collected in the external and internal parts of the stained glass windows of the Prebystery and Chapter House of the Pedralbes Monastery by using a precision (odontological) drill. These patinas were subsequently analyzed by X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR).

Results: XRD analyses evidenced the presence of sulfates (gypsum and thenardite), calcite, Ca-oxalates (whewellite and weddellite), and quartz forming part of the patinas. Although these mineral phases can be found in both color-type patinas, whewellite and thenardite are more common in the ochre-orange patinas. The results obtained were validated by the FTIR measurements. It has been observed, when thenardite is present, that gypsum occurs as traces. Thenardite is in most of the cases associated with whewellite and mainly occurs in the internal parts of the glass. In contrast, weddellite is limited to the absence of thenardite and whewellite and to the external parts of the stained glass. Quartz is present in all the patinas independent of their location and color. Calcite also occurs in many samples. It appears in both color-type patinas and, in some cases, is associated to the presence of weddellite but not to whewellite and/or thenardite.

Discussion: Glass composition together with environmental conditions and location of the patinas (internal or external parts of the stained glass window), as well as the provenance of the glass within the monastery, are the main factors that define the development of the new mineral phases. Moreover, the action of microorganisms, when present, can also strongly influence the development of some mineral phases. For example, the formation of calcite in the external parts of the stained glass (associated with the presence of oxalates) is related to the action of microorganisms. When calcite is formed in the internal parts of the glass and it is not associated with the presence of Ca-oxalates, an inorganic origin can be invoked. The presence of weddellite requires a very humid microenvironment with very little exposure to sunlight. In fact, this mineral phase has only been observed in the external parts of some glass located in the humid and shady side of the monastery. Whewellite (which only appears in the internal parts) needs a low degree of relative humidity. It has been observed that sulfur precipitating in basically one mineral phase (thenardite or gypsum) depends on the microenvironmental conditions of the moment and the glass composition. When thenardite occurs, it can be maintained that the original glass is of Na composition. The occurrence of quartz in all samples is interpreted as being due to the deposition of atmospheric particulate matter. The color of the patinas can be originated by different processes (presence of carotenes, organic pigmentation, atmospheric contamination, etc.).

Conclusions: In the case of moderately weathered stained glass windows, the combination of XRD and FTIR techniques is very useful to obtain a fast preliminary evaluation of the degree of weathering of a stained glass window. The presence of specific mineral phases in the patina (e.g., thenardite) confirms the Na composition of the original stained glass. This is important since Na-rich glass underwent a lesser degree of weathering than K- or K-Ca-rich glass. However, their absence cannot preclude other possibilities. It has been extensively evidenced through time that environmental conditions play an important role on the formation of the different mineral phases which form part of the patinas.

Recommendations And Perspectives: The first step in the restoration of a stained glass window is the evaluation of the degree of deterioration of the glass. This evaluation includes a chemical analysis of the glass as well as a characterization of the patinas developed on their surfaces. The obtained results will be essential in order to define the best restoration practices to be followed.

Download full-text PDF

Source
http://dx.doi.org/10.1007/s11356-008-0078-0DOI Listing

Publication Analysis

Top Keywords

stained glass
48
glass
26
mineral phases
24
environmental conditions
20
glass window
16
glass composition
16
internal parts
16
parts stained
16
external parts
16
patinas
15

Similar Publications

Investigate the impact of antimicrobial photodynamic therapy (aPDT) using different photosensitizers (PSs) such as indocyanine green (IG), curcumin (CC), and methylene blue (MB), with or without intracanal application of calcium hydroxide (CH), on the push-out bond strength of glass-fiber posts (GFPs) to intraradicular dentin, the chemical composition of the root substrate, and the sealing of the adhesive interface across different thirds of intraradicular dentin. A total of 112 bovine teeth underwent biomechanical preparation and were divided into eight experimental groups (n = 14 each): Negative control with deionized water; positive control with deionized water + CH; IG group with indocyanine green and infrared laser; IG + CH group; CC group with curcumin and blue LED; CC + CH group; MB group with methylene blue and red laser; and MB + CH group. The push-out bond strength was measured using a universal testing machine (n = 8), and scanning electron microscopy characterized the fracture patterns.

View Article and Find Full Text PDF

The Effect of Plaque Detectors on the Color Stability of Two Types of Restorative Materials.

J Esthet Restor Dent

January 2025

Department of Biomedical and Neuromotor Science (DIBINEM), Alma Mater Studiorum, University of Bologna, Bologna, Italy.

Objective: To investigate the color stability of a one-shade resin-based composite material (RC) and a glass-ionomer cement (GIC) after staining with plaque detectors (PDs) with different formulations and delivery forms.

Materials And Methods: Rectangular-shaped specimens (7 × 3 × 2 mm) were produced with RC (Venus Diamond One, Kulzer) and GIC (Fujy IX GP, GC) (n = 30). Further, the following PDs were used on the specimens: (1) tablets (T; Plaq-Search, TePe); (2) mouthwash (M; Plaque Agent, Miradent); and (3) light-curing liquid (L; Plaque test, Ivoclar).

View Article and Find Full Text PDF

Recently, 3-D porous architecture of the composites play a key role in cell proliferation, bone regeneration, and anticancer activities. The osteoinductive and osteoconductive properties of β-TCP allow for the complete repair of numerous bone defects. Herein, β-TCP was synthesized by wet chemical precipitation route, and their 3-D porous composites with HBO and Cu nanoparticles were prepared by the solid-state reaction method with improved mechanical and biological performances.

View Article and Find Full Text PDF

Background: Uveal melanoma (UM) is the most common primary intraocular malignancy in adults. The median overall survival time for patients who develop metastasis is approximately one year. In this study, we aim to leverage deep learning (DL) techniques to analyze digital cytopathology images and directly predict the 48 month survival status on a patient level.

View Article and Find Full Text PDF

Giant unilamellar vesicles (GUVs) are versatile cell models in biomedical and environmental research. Of the various GUV production methods, hydrogel-assisted GUV production is most easily implemented in a typical biological laboratory. To date, agarose, polyvinyl alcohol, cross-linked dextran-PEG, polyacrylamide, and starch hydrogels have been used to produce GUVs.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!