[Microtensile bond strengths of one-step self-etching adhesive systems].

Zhonghua Kou Qiang Yi Xue Za Zhi

Department of Cariology and Endodontology, Peking University School and Hospital of Stomatology, Beijing 100081, China.

Published: April 2007

Objective: To evaluate the microtensile bond strength of one-step self-etching adhesives to dentin in vitro.

Methods: Three commercially available one-step self-etching bonding systems (group A: Adper Prompt, group B: Clearfil S(3) Bond, group C: Xeno III) were compared with two-step self-etching adhesive (group D: Clearfil SE Bond) in this study. The microtensile bond strength was determined with microtensile tester and the fractured bonding surfaces were observed under stereomicroscope and scanning electronic microscope (SEM). The mean bond strengths were analyzed using one-way ANOVA test (P < 0.05).

Results: Mean microtensile bond strengths of group C, B, A and D were (34.59 +/- 3.46), (30.46 +/- 3.82), (23.36 +/- 2.55) and (45.06 +/- 5.29) MPa, respectively. Group D showed the highest bond strength (P < 0.01).

Conclusions: Two-step self-etching adhesive had a higher bond strength than one-step self-etching adhesive systems, although all of them can satisfy the clinical requirements.

Download full-text PDF

Source

Publication Analysis

Top Keywords

one-step self-etching
16
self-etching adhesive
16
bond strength
16
bond strengths
12
microtensile bond
12
bond
8
strength one-step
8
group clearfil
8
clearfil bond
8
two-step self-etching
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!