Much evidence suggests that ultra high molecular weight polyethylene (UHMWP) irradiated to 9.5 Mrad has lower wear than UHMWP given 5 Mrad. Curiously, highly cross-linked polyethylenes gain weight during hip simulator testing. We postulated that (a) UHMWP irradiated to 9.5 Mrad would wear less than UHMWP irradiated to 5 Mrad UHMWP, (b) articulation against 38-mm heads would accentuate this difference, and (c) weight gain of highly cross-linked material reflects the inadequacy of load soak controls. We compared 9.5 versus 5 Mrad polyethylene in hip simulator wear tests, with both load soak corrections and with novel "motion soak" corrections. The 9.5-Mrad material wore less than 5-Mrad material for 32- and 38-mm heads. Motion soak corrections were more accurate than load soak corrections.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.arth.2006.07.009DOI Listing

Publication Analysis

Top Keywords

hip simulator
12
highly cross-linked
12
uhmwp irradiated
12
irradiated mrad
12
load soak
12
soak corrections
12
simulator wear
8
ultra high
8
high molecular
8
molecular weight
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!