Dome-shaped gold nanoparticles (with an average diameter of 10.5 nm) are grown on H-terminated Si(100) substrates by simple techniques involving electro- and electroless deposition from a 0.05 mM AuCl3 and 0.1 M NaClO4 solution. XPS depth profiling data (involving Au 4f core-level and valence band spectra) reveal for the first time the formation of gold silicide at the interface between the Au nanoparticles and Si substrate. UV-visible diffuse reflectance spectra indicate that both samples have surface plasmon resonance maxima at 558 nm, characteristic of an uniform distribution of Au nanoscale particles of sufficiently small size. Glancing-incidence XRD patterns clearly show that the deposited Au nanoparticles belong to the fcc phase, with the relative intensity of the (220) plane for Au nanoparticles obtained by electroless deposition found to be notably larger than that by electrodeposition.

Download full-text PDF

Source
http://dx.doi.org/10.1021/ja070441jDOI Listing

Publication Analysis

Top Keywords

electroless deposition
12
gold nanoparticles
8
h-terminated si100
8
electro- electroless
8
nanoparticles
5
interfacial bonding
4
bonding gold
4
nanoparticles h-terminated
4
si100 substrate
4
substrate electro-
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!