Purpose: The purpose of this in vitro study is to find the best parameters in detecting the casting defects made of titanium, nickel-chromium and chromium-cobalt using dental X ray machine.
Methods: Casting sheets in different thickness (1.0 mm, 0.6 mm, 0.3 mm)were fabricated using of Ti, Ni-Cr and Cr-Co.Small pores on the surfaces were made with laser welder to simulate the internal porosity of the castings. Parameters of the dental X ray machine were adjusted to take films. The data were analyzed using SPSS12 software package for group t test.
Results: The thickness of Ti had no significant effect on the setting of the parameters of the dental X ray machine in detecting the defects of titanium castings (P>0.05), while the thickness of Ni-Cr and Cr-Co had significant effect on the setting of the parameters (P<0.05).
Conclusion: Dental X ray machine can be used in detecting the defects of titanium casting sheets.
Download full-text PDF |
Source |
---|
Adv Colloid Interface Sci
January 2025
Department of Biotechnology, School of Applied Sciences and Technology, BLDE (Deemed to be University), Bangaramma Sajjan Campus, Vijayapura 586103, India; Department of Basic Sciences, Faculty of Engineering and Technology, CMR University, Bangalore 562149, India. Electronic address:
Biosurfactants are biodegradable, non-toxic, and environmentally beneficial substances that are produced by microorganisms. Due to their chemical characteristics and stability in various environmental circumstances, biosurfactants are low-molecular-weight, surface-active molecules of great industrial importance. The choice of the producer microbe, kind of substrate, and purification technique determine the chemistry of a biosurfactant and its production cost.
View Article and Find Full Text PDFCureus
December 2024
Department of Dental Sciences, Faculty of Medicine, University of Liege, Liege, BEL.
Background Fracture of nickel-titanium (Ni-Ti) instruments in root canals is commonly associated with compromised outcomes in endodontic treatment. There is no single, universally accepted approach for managing this complication. The objective of this study is to evaluate the effectiveness of an Nd: YAP laser-assisted protocol in removing fractured Ni-Ti files in teeth with minimal root curvature (less than 15 degrees).
View Article and Find Full Text PDFPeerJ
January 2025
Department of Organismal Biology, Uppsala University, Uppsala, Sweden.
In this study, we attempt to illustrate fossil vertebrate dental tissue geochemistry and, by inference, its extent of diagenetic alteration, using quantitative, semi-quantitative and optical tools to evaluate bioapatite preservation. We present visual comparisons of elemental compositions in fish and plesiosaur dental remains ranging in age from Silurian to Cretaceous, based on a combination of micro-scale optical cathodoluminescence (CL) observations (optical images and scanning electron microscope) with minor, trace and rare earth element (REE) compositions (EDS, maps and REE profiles), as a tool for assessing diagenetic processes and biomineral preservation during fossilization of vertebrate dental apatite. Tissue-selective REE values have been obtained using laser ablation-inductively coupled plasma-mass spectrometry (LA-ICP-MS), indicating areas of potential REE enrichment, combined with cathodoluminescence (CL) analysis.
View Article and Find Full Text PDFOper Dent
January 2025
*Kraig S. Vandewalle, DDS, MS, Col (ret), USAF, DC, Air Force Consultant in Dental Research Advanced Education in General Dentistry Residency, AF Postgraduate Dental School, Joint Base San Antonio - Lackland, TX, USA; Uniformed Services University of the Health Sciences, Bethesda, MD, USA.
Objective: The purpose of this study was to compare the optical, mechanical, and biological properties of two new, inexpensive lithium disilicate (LS2) materials (Lodden (LOD), LD Medical Technology; and BeautyZir (BZ), BeautyZir Technology) to a clinically established LS2 material (IPS e.max CAD (EMAX), Ivoclar Vivadent).
Methods And Materials: The optical properties of the translucency parameter (TP) and opalescence parameter (OP) were obtained with a dental spectrophotometer.
J Dent Educ
January 2025
Department of Community Oral Health, Faculty of Dentistry, SEGi University, Kota Damansara, Petaling Jaya, Selangor, Malaysia.
Objectives: Intraoral periapical radiographic techniques are mandatory exercises taught to undergraduate students during their training. The key challenges encountered while teaching the bisecting angle technique (BAT) include correctly positioning the X-ray cone and adjusting the central X-ray beam to the tooth of interest. To address this, a custom-designed pointed laser light (CDPLL) was fabricated and attached to the X-ray cone.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!