Purpose: The purpose of this study was to determine the roles of alginate composition and gelling cations on bead swelling, which affects its durability.

Method: Using a 2-channel droplet generator, microspheres were generated with 1.5% solutions of low viscosity high-mannuronic acid (LVM), medium viscosity high-mannuronic acid (MVM), low viscosity high-guluronic acid (LVG) and medium viscosity high-guluronic acid (MVG) alginate. They were gelled by cross-linking with 1.1% solution of either BaCl2 or CaCl2. The diameters of the micro-beads were measured and recorded on day 0. The micro-beads were subsequently washed and incubated in saline at 37 degrees C for 2 weeks with size assessment every 2 days. The data were normalized by calculation of the percentage change from control (day 0) for all groups of micro-beads.

Results: Diameters of all beads were between 550 and 700 microm on day 0. Viscosity had no effect on swelling of Ba++- and Ca++-alginate micro-beads. Ca++-alginate micro-beads were more prone to swelling than the corresponding Ba++-alginate beads. High G-Ba++ beads had only a modest increase in size over time, in contrast to the high M-Ba++.

Conclusion: Alginate composition and the gelling cation have significant effects on bead swelling.

Download full-text PDF

Source
http://dx.doi.org/10.1080/02652040500286144DOI Listing

Publication Analysis

Top Keywords

alginate composition
12
composition gelling
12
gelling cation
8
bead swelling
8
low viscosity
8
viscosity high-mannuronic
8
high-mannuronic acid
8
medium viscosity
8
viscosity high-guluronic
8
high-guluronic acid
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!