The purpose of the present study was to evaluate the bond strength and durability of four bonding systems joined to a prefabricated porcelain material (Vita Celay Blanks). Two sizes of porcelain block were bonded with one of the following systems: (1) Clapearl Bonding Agent and Clapearl DC; (2) Imperva Porcelain Primer and Imperva Dual; (3) Monobond S and Variolink II; or (4) Tokuso Ceramics Primer and Bistite II. Shear bond strength was measured after 24-hour immersion in water and after subsequent thermocycling. The average pre- and post-thermocycling bond strengths in MPa (n=8) were: 52.5 and 42.5 for bonding system (1), 47.7 and 32.8 for (2), 55.0 and 48.8 for (3), and 51.5 and 25.6 for (4). Although prethermocycling results were not statistically different from each other, Group (3) exhibited the greatest strength after thermocycling.

Download full-text PDF

Source
http://dx.doi.org/10.4012/dmj.24.257DOI Listing

Publication Analysis

Top Keywords

bonding systems
8
prefabricated porcelain
8
porcelain material
8
bond strength
8
effectiveness bonding
4
bonding
4
systems bonding
4
bonding durability
4
durability prefabricated
4
porcelain
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!