We report a systematic increase of the superconducting transition temperature T(c) with a biaxial tensile strain in MgB2 films to well beyond the bulk value. The tensile strain increases with the MgB2 film thickness, caused primarily by the coalescence of initially nucleated discrete islands (the Volmer-Weber growth mode.) The T(c) increase was observed in epitaxial films on SiC and sapphire substrates, although the T(c) values were different for the two substrates due to different lattice parameters and thermal expansion coefficients. We identified, by first-principles calculations, the underlying mechanism for the T(c) increase to be the softening of the bond-stretching E(2g) phonon mode, and we confirmed this conclusion by Raman scattering measurements. The result suggests that the E(2g) phonon softening is a possible avenue to achieve even higher T(c) in MgB2-related material systems.

Download full-text PDF

Source
http://dx.doi.org/10.1103/PhysRevLett.93.147006DOI Listing

Publication Analysis

Top Keywords

superconducting transition
8
transition temperature
8
tensile strain
8
e2g phonon
8
enhancement superconducting
4
temperature mgb2
4
mgb2 strain-induced
4
strain-induced bond-stretching
4
bond-stretching mode
4
mode softening
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!