The effect of matrix selection, filler composition, filler silanization, operator variations, and test site (dental clinic) on the wear rate of eight composites were evaluated. The wear was measured on replicas using both a microscopic and a laser scanning measuring method. The average wear rate on contact-free surfaces was 9.2 +/- 4.2 microm/month with the microscopic measurement and 8.5 +/- 3.7 microm/ month with the laser scanner over the 36-month period. The urethane-based composites performed significantly better than those which were bisGMA-based. Restorations placed at one dental clinic showed significantly lower initial wear. There was also a significant difference between the operators that was most pronounced during the first 6 months. The other variable (filler composition and silane treatment) did not affect the wear rate significantly.

Download full-text PDF

Source
http://dx.doi.org/10.1034/j.1600-0722.2001.00064.xDOI Listing

Publication Analysis

Top Keywords

wear rate
12
filler composition
8
dental clinic
8
wear
5
clinical wear
4
wear performance
4
performance experimental
4
experimental dental
4
dental composites
4
composites three
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!