Hua Xi Kou Qiang Yi Xue Za Zhi
December 2020
Objective: This study aimed to investigate the effect of occlusal thickness design on fracture resistance of endocrowns restored with lithium disilicate ceramic and zirconia.
Methods: A total of 24 artificial first mandibular molars were randomly divided into four groups with six teeth in each group as follows: group lithium disilicate ceramic-2 mm (lithium disilicate ceramic, with an occlusal thickness of 2 mm and a retainer length of 4 mm); group lithium disilicate ceramic-4 mm (lithium disilicate ceramic, with an occlusal thickness of 4 mm and a retainer length of 2 mm); group zirconia-2 mm (zirconia, with an occlusal thickness of 2 mm and a retainer length of 4 mm); and group zirconia-4 mm (zirconia, with an occlusal thickness of 4 mm and a retainer length of 2 mm). After adhesive cementation (RelyX Ultimate Clicker), all specimens were subjected to thermocycling (10 000 cycles).