J Nanosci Nanotechnol
February 2016
In this work, hydrogen production from glycerol by steam reforming was studied using Ni-metal oxide catalysts. Ni-based catalyst becomes deactivated during steam reforming reactions because of coke deposits and sintering. Therefore, the aim of this study was to reduce carbon deposits and sintering on the catalyst surface by adding a promoter.
View Article and Find Full Text PDFJ Nanosci Nanotechnol
January 2015
In this work, hydrogen production from glycerol by Steam Reforming (SR) was studied by Ni-Ce catalysts supported on LaAlO3 perovskite in order to effect of the cerium loading amount and the reaction conditions. Nano size Ni-Ce/LaAlO3 catalysts were prepared by precipitation method. The structure of the catalysts was characterized by XRD analysis.
View Article and Find Full Text PDF