Aim: to compare the levels of IFN-γ, TGF-β and C-reactive protein (CRP) in healthy patients (HP) and chronic periodontitis patients (CP) before and seven days after the last session of Non-Surgical Periodontal Treatment (NSPT). Materials and Methods: 40 subjects were divided into two groups: healthy (n= 20), and with chronic periodontitis (n = 20). Serum and gingival crevicular fluid (GCF) were collected from each patient and quantified for IFN-γ, TGF-β and CRP using the enzyme-linked immunosorbent assay (ELISA).
View Article and Find Full Text PDFObjective: To investigate the effect of collagen cross-links on the stability of adhesive properties, the degree of conversion within the hybrid layer, cytotoxicity and the inhibition potential of the MMPs' activity.
Methods: The dentin surfaces of human molars were acid-etched and treated with primers containing: 6.5wt% proanthocyanidin, UVA-activated 0.
This study evaluated the influence of an alternative surface treatment on the microshear bond strength (μsbs) of zirconia-based ceramic. Thirty-five zirconia disks were assigned to five groups according to the following treatments: Control (CO), glass and silane were not applied to the zirconia surface; G1, air blasted with 100μm glass beads + glaze + silane; G2, a gel containing 15% (by weight) glass beads applied to the ceramic surface + glaze + silane; G3, a gel containing 25% (by weight) glass beads applied to the ceramic surface + glaze + silane; and G4, a gel containing 50% (by weight) glass beads applied to the ceramic surface + glaze + silane. The specimens were built up using RelyX ARC®, according to the manufacturer's recommendations, and inserted in an elastomeric mold with an inner diameter of 0.
View Article and Find Full Text PDFPurpose: To evaluate the effects of an electric current-assisted application on the bond strength and interfacial morphology of self-adhesive resin cements bonded to dentin.
Methods: Indirect resin composite build-ups were luted to prepared dentin surfaces using two self-adhesive resin cements (RelyX Unicem and BisCem) and an ElectroBond device under 0, 20, or 40 μA electrical current. All specimens were submitted to microtensile bond strength test and to interfacial SEM analysis.