Background: The aim of this study was evaluated the eroded enamel rehardening potential using upper palatal and lower buccal removable appliances in different times of salivary exposure (30 min, 1h, 2h, 12h) after a single erosive challenge event.
Material And Methods: After initial surface hardness evaluation, bovine enamel blocks were eroded in vitro (0.01 M hydrochloric acid, pH 2.
This in vitro study evaluated the impact of initial erosion on the susceptibility of enamel to further erosive challenge. Thirty bovine enamel blocks were selected by surface hardness and randomized into two groups (n = 15): GC- group composed by enamel blocks without erosion lesion and GT- group composed by enamel blocks with initial erosion lesion. The baseline profile of each block was determined using the profilometer.
View Article and Find Full Text PDFObjectives: The aim of this study was to evaluate the effect of removing excess of resin-based materials applied to eroded enamel, subjected to erosive challenge.
Methods: Bovine enamel blocks were immersed in HCl 0.01M, pH 2.
Objective: The present study analyzed xylitol concentrations in artificial saliva over time after application of varnishes containing 10% and 20% xylitol.
Material And Methods: Fifteen bovine enamel specimens (8x4 mm) were randomly allocated to 3 groups (n=5/group), according to the type of varnish used: 10% xylitol, 20% xylitol and no xylitol (control). After varnish application (4 mg), specimens were immersed in vials containing 500 µL of artificial saliva.