This paper assesses the effects of light characteristics and irradiation time on the Vickers microhardness (VH) of a dual-photoinitiator commercial composite and on temperature increase in the pulp chamber (deltaT). Four recent light-emitting diodes (LEDs)--bluephaseG2 (BG2), bluephase16i (B16i), G-Light (G) and Freelight2 (F2)--and one control halogen light (XL3000-X) were tested on two shades of Tetric EvoCeram (A2 and Bleach XL), whose respective commercial formulations differed based on their concentration of camphorquinone and lucirin TPO. Three different irradiation times were applied--10, 20 and 40 seconds-and VH was measured on the upper and lower surfaces of 2-mm thick samples.