Objective: To evaluate the microtensile bond strength of four dental computer-aided design/computer-aided manufactured (CAD/CAM) ceramics after application of four different surface treatments.
Materials And Methods: Four dental CAD/CAM ceramics were tested: feldspathic ceramic (VITABLOCKS-Mark II), polymer-infiltrated ceramic network (VITA ENAMIC), zirconia-reinforced lithium silicate (VITA SUPRINITY), and yttria-stabilized zirconia (VITA YZ T). Four surface treatments were applied: no treatment, 5% hydrofluoric acid-etching, airborne particle abrasion, and tribochemical silica coating.