Herein, we report a study on the preparation, properties, and depolymerization of pristine and vulcanized poly(cyclopentene) (poly(CP)), poly(norbornene--cyclopentene) (poly(NB--CP)) and poly(-dicyclopentadiene--cyclopentene) (poly (DCP--CP)). First, poly(CP), poly(NB--CP) and poly(DCP--CP) were prepared with high molecular weight control ( = 200 000-500 000) using dichloro(3-phenyl-1-inden-1-ylidene)bis(tricyclohexylphosphine)ruthenium(ii). Next, carbon black, zinc oxide and other additives were blended into the pristine polymers using a mixer and twin roll rubber mills at 50 °C, followed by vulcanization in metal molds at 160 °C for 10 min, resulting in molded black rubber specimens.