Many current controlled-release fertilizers (CRFs) are coated with nonbiodegradable polymers that can contribute to microplastic pollution. Here, coatings of self-immolative poly(ethyl glyoxylate) (PEtG) capped with a carbamate and blended with polycaprolactone (PCL) or poly(l-lactic acid) (PLA) were evaluated. They were designed to depolymerize and release fertilizers in the vicinity of plant roots, where the pH is lower than that in the surrounding environment.
View Article and Find Full Text PDFPolymeric coatings are commonly employed to alter surface properties. While some coatings are designed to remain stable over a prolonged period, in applications such as pharmaceuticals or fertilizers, the coating is designed to erode and reveal or release the underlying material. Self-immolative polymers (SIPs) undergo depolymerization following the cleavage of stimuli-responsive end-caps from their termini, enabling controlled depolymerization in the solid state and in solution.