Objective: This study evaluated the degree of conversion (DC), polymerization kinetics, and temperature of a new self-cure bulk-fill resin-based composite (Stela Automix, SDI).
Methods: The study was divided into seven groups: (1) Stela Primer, (2) Stela Automix, (3) Stela Automix exposed to light for 20 s after 100 s, (4) Stela Primer with Stela Automix, (5) Stela Primer with Stela Automix and exposed to light for 20 s after 100 s, (6) Scotchbond Universal with Stela Automix, and (7) Scotchbond Universal with Stela Automix and exposed to light for 20 s after 100 s. The real-time reaction rates and DC at the bottom of 2 mm thick specimens at ∼32 °C were measured at 720 s after insertion using a spectrometer with an Attenuated Total Reflectance detector.
Materials (Basel)
September 2024
Identifying the boundary between the tooth and the resin-based composite (RBC) is difficult when replacing restorations. Ultraviolet (UV) light has been reported to assist the viewer by causing the RBC to fluoresce. Using a laboratory-grade fiberoptic spectrometer, 46 RBCs were exposed to UV light from the Woodpecker O-Star curing light.
View Article and Find Full Text PDF