Hollow-fiber membranes for nanofiltration were prepared from the blending of Poly (ethylene glycol) (PEG) with Poly (vinyl chloride) (PVC) with different PEG molecular weights (400 and 4000 g/mol) and PVC via a dry/wet spinning process. In the spinning process, the effects of air gap, wind-up speed, dope extrusion rate, and bore extrusion rate were examined. In addition, the different lengths of the center tube, which acted as the inner-side fiber diameter during the preparation of hollow-fiber membranes, were studied.