The wear of ultra-high molecular weight polyethylene (UHMWPE) acetabular components in total hip replacements (THRs) has been shown to be highly dependent on the direction of shear. Greatly reduced wear rates have been reported for unidirectional, compared to multidirectional, articulation in vitro. This work for the first time enables investigation of a relationship between clinical wear conditions, as determined by patient gait path, and the mechanical and structural changes that occur within the UHMWPE acetabular component.